Final Magnetic Moment0.374 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.198 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.226 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.73 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi3Mn3(PO4)4 + MnCO3 + MnO2 + CO2 + Li3PO4 |
Band Gap2.267 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 0 0> | 195.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 274.2 |
AlN (mp-661) | <1 0 0> | <1 1 -1> | 237.5 |
BaF2 (mp-1029) | <1 0 0> | <1 0 -1> | 82.2 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 175.7 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 164.5 |
GaN (mp-804) | <1 0 1> | <1 1 1> | 245.5 |
GaAs (mp-2534) | <1 0 0> | <1 0 -1> | 164.3 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 325.1 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 329.1 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 325.1 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 274.2 |
KCl (mp-23193) | <1 0 0> | <1 0 -1> | 82.2 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 175.7 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 325.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 -1> | 164.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 329.1 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 87.9 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 260.0 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 263.6 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 195.0 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 274.2 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 175.7 |
YVO4 (mp-19133) | <1 0 1> | <0 1 1> | 203.5 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 65.0 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 130.0 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 263.6 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 329.1 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 274.2 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 274.2 |
BN (mp-984) | <1 0 1> | <1 0 0> | 260.0 |
Bi2Se3 (mp-541837) | <1 0 1> | <0 1 0> | 257.1 |
MoS2 (mp-1434) | <0 0 1> | <1 0 -1> | 246.5 |
MoS2 (mp-1434) | <1 0 0> | <0 0 1> | 274.2 |
MoS2 (mp-1434) | <1 0 1> | <0 0 1> | 274.2 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 65.0 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 219.4 |
CdTe (mp-406) | <1 1 0> | <1 0 -1> | 246.5 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 195.0 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 1> | 175.7 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 195.0 |
CdTe (mp-406) | <1 0 0> | <1 0 1> | 87.9 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 257.1 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 219.4 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 260.0 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 325.1 |
TiO2 (mp-2657) | <1 1 0> | <1 0 1> | 175.7 |
MgO (mp-1265) | <1 0 0> | <1 0 -1> | 164.3 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 219.4 |
C (mp-66) | <1 0 0> | <1 0 -1> | 164.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Hg2SeO5 (mp-30123) | 0.7498 | 0.000 | 3 |
Li3Fe3(BO3)4 (mp-767662) | 0.7143 | 0.362 | 4 |
Na3Ca(BO2)5 (mp-542719) | 0.6970 | 0.000 | 4 |
Li3B5(HO5)2 (mp-707105) | 0.7041 | 0.000 | 4 |
Na3Ca(BO2)5 (mp-614628) | 0.6722 | 0.002 | 4 |
Li3Ni(BO2)5 (mp-771081) | 0.6930 | 0.092 | 4 |
Li5Mn2P2(CO7)2 (mp-771378) | 0.1028 | 0.047 | 5 |
Li5Mn2P2(CO7)2 (mp-770318) | 0.2266 | 0.043 | 5 |
Li5Mn2P2(CO7)2 (mp-770317) | 0.1619 | 0.180 | 5 |
Li5Mn2P2(CO7)2 (mp-770310) | 0.2080 | 0.120 | 5 |
Li5Mn2P2(CO7)2 (mp-770157) | 0.2025 | 0.104 | 5 |
Li12Mn3VP4(CO7)4 (mp-767666) | 0.2976 | 0.054 | 6 |
Li12Fe3NiP4(CO7)4 (mp-767852) | 0.3016 | 0.166 | 6 |
Li12MnCo3P4(CO7)4 (mp-767749) | 0.2978 | 0.044 | 6 |
Li12VCr3P4(CO7)4 (mp-767735) | 0.3037 | 0.075 | 6 |
Li6VCrP2(CO7)2 (mp-767288) | 0.2987 | 0.080 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv P C O |
Final Energy/Atom-6.7273 eV |
Corrected Energy-362.7513 eV
-362.7513 eV = -336.3638 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|