Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.969 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.039 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.38 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBi2(SO4)3 + Na2SO4 + CO2 + Bi2CO5 |
Band Gap3.738 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 1> | <1 1 0> | 257.3 |
AlN (mp-661) | <0 0 1> | <1 0 1> | 313.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 202.5 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 234.9 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 199.9 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 162.0 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 67.5 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 283.5 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 171.5 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 54.0 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 215.9 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 121.5 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 323.8 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 243.0 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 202.4 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 171.5 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 283.5 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 121.5 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 135.0 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 54.0 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 323.8 |
ZnSe (mp-1190) | <1 0 0> | <0 1 1> | 67.5 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 283.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 161.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 67.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 283.5 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 324.0 |
LiF (mp-1138) | <1 0 0> | <0 1 1> | 67.5 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 161.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 283.5 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 202.5 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 333.2 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 121.5 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 283.5 |
YVO4 (mp-19133) | <0 0 1> | <1 0 1> | 156.6 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 133.3 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 66.6 |
TePb (mp-19717) | <1 0 0> | <1 1 0> | 85.8 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 333.2 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 283.5 |
Ag (mp-124) | <1 0 0> | <1 1 0> | 85.8 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 121.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 283.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 333.2 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 333.2 |
BN (mp-984) | <0 0 1> | <0 0 1> | 202.5 |
BN (mp-984) | <1 0 0> | <0 0 1> | 283.5 |
BN (mp-984) | <1 1 1> | <0 0 1> | 243.0 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 283.5 |
LiNbO3 (mp-3731) | <1 1 0> | <1 1 0> | 257.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Al2Si2H4O9 (mp-721216) | 0.7146 | 0.013 | 4 |
RuC4(O2F3)2 (mp-542700) | 0.6638 | 0.146 | 4 |
CaGaBO4 (mp-557855) | 0.6521 | 0.000 | 4 |
Al2Si2H4O9 (mp-541152) | 0.7058 | 0.013 | 4 |
MnZnPO5 (mvc-3247) | 0.7042 | 0.029 | 4 |
NaSbCSO7 (mp-768656) | 0.3226 | 0.036 | 5 |
NaBiPCO7 (mp-768122) | 0.3018 | 0.070 | 5 |
NaBiAsCO7 (mp-768996) | 0.3039 | 0.070 | 5 |
NaSbPCO7 (mp-768121) | 0.3773 | 0.101 | 5 |
NaCePCO7 (mp-767538) | 0.3618 | 0.029 | 5 |
NaLiMnPCO7 (mp-763833) | 0.6219 | 0.000 | 6 |
CdRe2H8C2(N2O5)2 (mp-733848) | 0.5658 | 0.016 | 6 |
BH6Ru3C6O19F4 (mp-699265) | 0.7228 | 0.645 | 6 |
CuP2H8CN2O5 (mp-24145) | 0.6085 | 0.288 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Bi C S O |
Final Energy/Atom-6.2989 eV |
Corrected Energy-149.7354 eV
-149.7354 eV = -138.5765 eV (uncorrected energy) - 11.1590 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)