Final Magnetic Moment0.917 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.296 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.046 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.06 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiCuO2 + CuO + NiO |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 308.6 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 308.6 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 246.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 123.5 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 246.9 |
AlN (mp-661) | <1 1 1> | <1 1 1> | 195.6 |
CeO2 (mp-20194) | <1 1 0> | <1 0 -1> | 216.8 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 156.7 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 187.5 |
GaN (mp-804) | <1 1 0> | <1 0 -1> | 271.1 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 61.7 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 219.3 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 282.0 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 244.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 54.2 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 219.3 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 31.3 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 282.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 31.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 156.7 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 313.3 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 250.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 156.7 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 187.5 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 250.7 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 282.0 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 156.7 |
Ag (mp-124) | <1 1 1> | <0 1 1> | 246.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 156.7 |
BN (mp-984) | <1 0 0> | <1 0 0> | 94.0 |
BN (mp-984) | <1 0 1> | <1 0 0> | 219.3 |
MoS2 (mp-1434) | <1 1 0> | <1 0 1> | 244.5 |
Al (mp-134) | <1 1 0> | <1 0 0> | 156.7 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 250.0 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 31.3 |
TeO2 (mp-2125) | <0 1 0> | <1 0 -1> | 271.1 |
TeO2 (mp-2125) | <0 1 1> | <1 0 0> | 156.7 |
TeO2 (mp-2125) | <1 0 0> | <1 0 -1> | 271.1 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 308.6 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 31.3 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 31.3 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 185.2 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 282.0 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 156.7 |
GaN (mp-804) | <0 0 1> | <1 0 -1> | 54.2 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 308.6 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 156.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 31.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 219.3 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 -1> | 54.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiCuO2 (mp-9158) | 0.5008 | 0.000 | 3 |
MgCuO2 (mvc-4732) | 0.5307 | 0.084 | 3 |
LiAgO2 (mp-996992) | 0.4970 | 0.022 | 3 |
Li5NbO5 (mp-770649) | 0.5507 | 0.021 | 3 |
CaCrO2 (mvc-2945) | 0.5375 | 0.108 | 3 |
Li3Ti(CuO2)4 (mp-772309) | 0.3667 | 0.063 | 4 |
Li3Co(CuO2)4 (mp-770184) | 0.3767 | 0.042 | 4 |
Li3Cr(CuO2)4 (mp-769804) | 0.1777 | 0.032 | 4 |
Li5NiO3F2 (mp-764683) | 0.4627 | 0.093 | 4 |
Li3Cu4SnO8 (mp-756288) | 0.4144 | 0.049 | 4 |
Fe3O4 (mp-715275) | 0.7046 | 0.748 | 2 |
Ti7O8 (mp-779692) | 0.7278 | 0.116 | 2 |
Fe3O4 (mp-715614) | 0.7103 | 0.468 | 2 |
Fe3O4 (mp-18731) | 0.6259 | 0.109 | 2 |
Cr3O4 (mp-772696) | 0.7038 | 0.082 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Cu_pv Ni_pv O |
Final Energy/Atom-5.0273 eV |
Corrected Energy-88.2189 eV
-88.2189 eV = -80.4366 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction) - 2.1640 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)