Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.594 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.044 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.42 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAs2O3 + Ta2O5 |
Band Gap2.670 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnna [52] |
Hall-P 2a 2bc |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 251.4 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 71.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 251.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 27.9 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 83.8 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 196.2 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 180.1 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 142.2 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 55.9 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 223.5 |
ZnSe (mp-1190) | <1 1 0> | <0 1 1> | 331.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 240.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 307.3 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 307.3 |
LiF (mp-1138) | <1 1 1> | <0 1 1> | 264.8 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 251.4 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 307.3 |
Ag (mp-124) | <1 1 1> | <0 1 1> | 264.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 195.6 |
GaSe (mp-1943) | <1 0 1> | <1 1 0> | 266.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 195.6 |
BN (mp-984) | <1 0 0> | <1 1 0> | 177.5 |
BN (mp-984) | <1 0 1> | <0 1 1> | 264.8 |
Al (mp-134) | <1 1 0> | <0 1 1> | 331.0 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 139.7 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 1> | 198.6 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 195.6 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 139.7 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 223.5 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 307.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 83.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 111.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 213.4 |
CeO2 (mp-20194) | <1 1 1> | <0 1 1> | 198.6 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 266.3 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 71.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 307.3 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 266.3 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 142.2 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 279.4 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 27.9 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 139.7 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 331.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 195.6 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 130.8 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 331.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 307.3 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 251.4 |
LiF (mp-1138) | <1 0 0> | <1 1 1> | 186.1 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 331.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Nb2SbO6 (mp-755840) | 0.4937 | 0.066 | 3 |
GeWO4 (mp-770711) | 0.2441 | 0.071 | 3 |
SnWO4 (mp-19654) | 0.3911 | 0.020 | 3 |
Ta2SnO6 (mp-556489) | 0.4981 | 0.000 | 3 |
NbSbO4 (mp-3612) | 0.5344 | 0.000 | 3 |
CuSb(MoO4)2 (mp-622126) | 0.6422 | 0.043 | 4 |
LiV2OF5 (mp-777088) | 0.6438 | 0.063 | 4 |
AlV(WO4)2 (mvc-603) | 0.5601 | 0.167 | 4 |
AlNi(WO4)2 (mvc-613) | 0.5750 | 0.231 | 4 |
LiNi(WO4)2 (mp-25603) | 0.5672 | 0.090 | 4 |
Cr2F5 (mp-558380) | 0.6921 | 0.003 | 2 |
SbO2 (mp-560098) | 0.5975 | 0.001 | 2 |
SbO2 (mp-1819) | 0.5504 | 0.002 | 2 |
SbO2 (mvc-6570) | 0.6834 | 0.137 | 2 |
Ta2O5 (mp-10390) | 0.6980 | 0.014 | 2 |
Li7Zr3Nb(TeO6)4 (mp-766103) | 0.7406 | 0.012 | 5 |
Li3ZrNb(TeO6)2 (mp-754249) | 0.6857 | 0.021 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ta_pv As O |
Final Energy/Atom-8.1776 eV |
Corrected Energy-207.4979 eV
-207.4979 eV = -196.2613 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)