Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.563 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.025 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.32 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCaI2 + LaI3 |
Band Gap1.899 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 273.4 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 273.4 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 246.9 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 273.4 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 273.4 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 273.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 68.4 |
Bi2Te3 (mp-34202) | <1 0 0> | <0 0 1> | 136.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 205.1 |
GaSe (mp-1943) | <1 1 0> | <0 1 0> | 246.9 |
LaAlO3 (mp-2920) | <1 1 0> | <0 1 0> | 246.9 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 205.1 |
BaF2 (mp-1029) | <1 1 1> | <0 1 1> | 214.0 |
BN (mp-984) | <0 0 1> | <0 1 1> | 214.0 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 164.6 |
KCl (mp-23193) | <1 1 1> | <0 1 1> | 214.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 273.4 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 164.6 |
CdTe (mp-406) | <1 1 0> | <0 1 0> | 246.9 |
TeO2 (mp-2125) | <1 1 1> | <0 0 1> | 205.1 |
C (mp-66) | <1 1 0> | <0 1 0> | 164.6 |
LiTaO3 (mp-3666) | <0 0 1> | <0 1 0> | 164.6 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 205.1 |
InSb (mp-20012) | <1 1 0> | <0 1 0> | 246.9 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 273.4 |
PbSe (mp-2201) | <1 1 0> | <0 1 0> | 164.6 |
MoSe2 (mp-1634) | <1 0 0> | <0 0 1> | 205.1 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 273.4 |
Ga2O3 (mp-886) | <1 0 1> | <0 0 1> | 136.7 |
CdSe (mp-2691) | <1 1 0> | <0 1 0> | 164.6 |
MoSe2 (mp-1634) | <1 1 1> | <0 0 1> | 273.4 |
C (mp-48) | <0 0 1> | <0 1 0> | 246.9 |
ZrO2 (mp-2858) | <1 1 1> | <0 1 0> | 246.9 |
Si (mp-149) | <1 1 1> | <0 0 1> | 205.1 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 273.4 |
WSe2 (mp-1821) | <1 0 0> | <0 0 1> | 205.1 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 136.7 |
SiC (mp-8062) | <1 1 0> | <0 1 0> | 82.3 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 273.4 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 273.4 |
MgF2 (mp-1249) | <1 1 0> | <0 0 1> | 205.1 |
MgF2 (mp-1249) | <1 1 1> | <0 1 1> | 214.0 |
Cu (mp-30) | <1 1 0> | <0 1 0> | 164.6 |
GaSb (mp-1156) | <1 0 0> | <0 0 1> | 273.4 |
GaSb (mp-1156) | <1 1 0> | <0 1 0> | 164.6 |
CaF2 (mp-2741) | <1 1 1> | <0 0 1> | 205.1 |
Fe2O3 (mp-24972) | <1 1 0> | <0 1 0> | 246.9 |
ZnTe (mp-2176) | <1 0 0> | <0 0 1> | 273.4 |
ZnTe (mp-2176) | <1 1 0> | <0 1 0> | 164.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LaMgI5 (mp-756448) | 0.2643 | 0.031 | 3 |
NbTe5Pd (mp-28616) | 0.5690 | 0.021 | 3 |
LaMgI5 (mp-756578) | 0.4130 | 0.015 | 3 |
CaLaI5 (mp-772082) | 0.3348 | 0.025 | 3 |
Ca3Pb3I14 (mp-771827) | 0.5788 | 0.083 | 3 |
Ca3Fe2(RhO6)2 (mvc-14254) | 0.5831 | 0.234 | 4 |
Ca2FeRhO6 (mvc-14247) | 0.7175 | 0.299 | 4 |
Ca3Co2(RhO6)2 (mvc-14984) | 0.6953 | 0.189 | 4 |
SrLiFeF6 (mp-567062) | 0.7227 | 0.723 | 4 |
SrLiCoF6 (mp-567434) | 0.7144 | 0.017 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv La I |
Final Energy/Atom-3.6432 eV |
Corrected Energy-102.0088 eV
-102.0088 eV = -102.0088 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)