Final Magnetic Moment0.271 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.678 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.109 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.90 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToVPO4 + V2O3 + Li3PO4 + SiO2 |
Band Gap1.186 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPc [7] |
HallP 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 111.6 |
BaF2 (mp-1029) | <1 1 1> | <1 0 1> | 140.6 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 209.5 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 229.3 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 229.3 |
KCl (mp-23193) | <1 1 1> | <1 0 1> | 140.6 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 111.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 209.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 229.3 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 229.3 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 305.7 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 223.2 |
BN (mp-984) | <0 0 1> | <1 0 0> | 223.2 |
BN (mp-984) | <1 0 1> | <0 0 1> | 305.7 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 1> | 140.6 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 1> | 140.6 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 -1> | 129.7 |
Al (mp-134) | <1 1 0> | <0 0 1> | 229.3 |
Au (mp-81) | <1 1 0> | <1 0 0> | 223.2 |
CdSe (mp-2691) | <1 1 0> | <1 0 0> | 111.6 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 305.7 |
C (mp-48) | <1 0 1> | <0 0 1> | 305.7 |
C (mp-48) | <1 1 1> | <0 0 1> | 305.7 |
ZrO2 (mp-2858) | <0 1 0> | <0 0 1> | 305.7 |
CaCO3 (mp-3953) | <1 1 0> | <0 0 1> | 152.9 |
YAlO3 (mp-3792) | <0 1 1> | <1 0 1> | 140.6 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 152.9 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 152.9 |
PbSe (mp-2201) | <1 1 0> | <1 0 0> | 111.6 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 0> | 209.5 |
BaTiO3 (mp-5986) | <1 0 1> | <0 1 1> | 259.4 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 305.7 |
ZnO (mp-2133) | <1 1 0> | <0 0 1> | 152.9 |
GaSb (mp-1156) | <1 1 0> | <1 0 0> | 111.6 |
Cu (mp-30) | <1 1 0> | <1 0 0> | 111.6 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 229.3 |
Ga2O3 (mp-886) | <0 1 0> | <1 0 0> | 223.2 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 305.7 |
GaTe (mp-542812) | <0 0 1> | <1 0 0> | 223.2 |
GaTe (mp-542812) | <1 0 -1> | <1 0 0> | 223.2 |
LiAlO2 (mp-3427) | <1 0 0> | <0 0 1> | 229.3 |
Al2O3 (mp-1143) | <1 1 0> | <0 0 1> | 229.3 |
Al2O3 (mp-1143) | <1 1 1> | <0 0 1> | 229.3 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 229.3 |
ZnTe (mp-2176) | <1 1 0> | <1 0 0> | 111.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe4P2O9 (mp-637226) | 0.4143 | 0.391 | 3 |
Mn4P2O9 (mp-770499) | 0.4236 | 0.015 | 3 |
Cr4P2O9 (mp-773396) | 0.4414 | 0.230 | 3 |
Ni4P2O9 (mp-771899) | 0.4390 | 0.037 | 3 |
Na2W2O7 (mp-25800) | 0.4728 | 0.021 | 3 |
Li4FeP2O9 (mp-761506) | 0.3852 | 0.166 | 4 |
Li4V2(SiO4)3 (mp-770256) | 0.3764 | 0.086 | 4 |
Li3Mn(PO4)2 (mp-762881) | 0.2309 | 0.244 | 4 |
Li3Cr(PO4)2 (mp-774182) | 0.2569 | 0.058 | 4 |
Li3Fe(PO4)2 (mp-762816) | 0.3410 | 0.065 | 4 |
Li4Fe5P6WO24 (mp-775677) | 0.3912 | 0.316 | 5 |
Li4V2Si(PO6)2 (mp-770404) | 0.2468 | 0.077 | 5 |
Li4V2Si(PO6)2 (mp-770190) | 0.1776 | 0.258 | 5 |
Li4V2Si(PO6)2 (mp-778895) | 0.1434 | 0.123 | 5 |
Li4Mn5P6WO24 (mp-771110) | 0.3934 | 0.075 | 5 |
Li4CrCo2Ni3(PO4)6 (mp-776777) | 0.3968 | 0.086 | 6 |
Li4Mn2Fe3P6WO24 (mp-770860) | 0.4132 | 0.174 | 6 |
Li4Cr2Ni3Sn(PO4)6 (mp-778614) | 0.4156 | 0.184 | 6 |
Li4CrFe2Ni3(PO4)6 (mp-776753) | 0.4091 | 0.778 | 6 |
Li4Co2Ni3Sn(PO4)6 (mp-776757) | 0.4101 | 0.139 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv Si P O |
Final Energy/Atom-6.9469 eV |
Corrected Energy-630.7019 eV
-630.7019 eV = -583.5360 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction) - 13.4560 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)