Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.644 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.111 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.00 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFeH2SO5 + Li2SO4 + H2O |
Band Gap3.918 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 1 0> | 235.1 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 87.6 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 208.7 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 208.7 |
GaN (mp-804) | <1 0 1> | <1 0 -1> | 114.2 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 105.3 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 313.0 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 210.7 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 313.0 |
Al (mp-134) | <1 0 0> | <0 1 1> | 262.9 |
Al (mp-134) | <1 1 0> | <1 0 1> | 138.1 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 313.0 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 313.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 281.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 211.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 313.0 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 -1> | 114.2 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 208.7 |
TeO2 (mp-2125) | <1 0 1> | <0 1 0> | 156.5 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 281.6 |
SiC (mp-7631) | <1 0 0> | <1 0 -1> | 228.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 262.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 138.1 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 281.6 |
TiO2 (mp-2657) | <1 0 0> | <1 1 0> | 235.1 |
C (mp-66) | <1 1 0> | <0 1 0> | 260.9 |
GdScO3 (mp-5690) | <0 0 1> | <0 1 0> | 260.9 |
LiF (mp-1138) | <1 0 0> | <0 1 1> | 262.9 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 262.9 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 0> | 313.0 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 313.0 |
Mg (mp-153) | <1 0 1> | <1 0 -1> | 114.2 |
Mg (mp-153) | <1 1 1> | <0 1 0> | 208.7 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 281.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 70.4 |
BN (mp-984) | <1 1 0> | <0 1 0> | 104.3 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 211.2 |
BaTiO3 (mp-5986) | <1 1 0> | <0 1 1> | 262.9 |
BaTiO3 (mp-5986) | <1 1 1> | <0 1 0> | 313.0 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 281.6 |
NdGaO3 (mp-3196) | <0 1 0> | <0 1 0> | 208.7 |
NdGaO3 (mp-3196) | <1 1 1> | <0 1 0> | 208.7 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 -1> | 228.3 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 260.9 |
Si (mp-149) | <1 0 0> | <0 1 0> | 208.7 |
Au (mp-81) | <1 0 0> | <0 0 1> | 70.4 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 281.6 |
TiO2 (mp-2657) | <1 0 1> | <1 1 0> | 235.1 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 156.5 |
WS2 (mp-224) | <0 0 1> | <0 1 0> | 313.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AlTeI7 (mp-29407) | 0.7444 | 0.000 | 3 |
InTeI7 (mp-680058) | 0.7419 | 0.000 | 3 |
GaTeI7 (mp-29541) | 0.7481 | 0.000 | 3 |
CuH16(ClO8)2 (mp-705846) | 0.4603 | 0.046 | 4 |
Fe3P2(H2O3)4 (mp-745134) | 0.4832 | 0.186 | 4 |
Ca5As4(HO2)10 (mp-24436) | 0.4837 | 0.001 | 4 |
ZnH8SO8 (mp-24708) | 0.4688 | 0.016 | 4 |
Mn5P4(HO2)10 (mp-744430) | 0.4678 | 0.003 | 4 |
Li2NiH12(SO7)2 (mp-771658) | 0.2776 | 0.114 | 5 |
Li2CoH12(SO7)2 (mp-770638) | 0.3873 | 0.062 | 5 |
Na2NiH12(SO7)2 (mp-603679) | 0.3366 | 0.016 | 5 |
K2CoH12(SO7)2 (mp-549032) | 0.4167 | 0.000 | 5 |
K2CoH12(SO7)2 (mp-604610) | 0.4048 | 0.000 | 5 |
NaMnP2H10NO10 (mp-761339) | 0.6681 | 0.119 | 6 |
KNaZrSi3H4O11 (mp-773906) | 0.7073 | 0.000 | 6 |
NaCoBP2H2O9 (mp-601388) | 0.6335 | 0.072 | 6 |
Be2CoH20N2(O3F4)2 (mp-25732) | 0.7391 | 0.000 | 6 |
Ca2AlH8S2Cl(O6F)2 (mp-643446) | 0.7180 | 0.001 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv H S O |
Final Energy/Atom-5.3476 eV |
Corrected Energy-359.3335 eV
-359.3335 eV = -331.5496 eV (uncorrected energy) - 22.3180 eV (MP Anion Correction) - 5.4660 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)