Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.857 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.129 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.54 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFeH2SO5 + Li2SO4 + H2O |
Band Gap4.237 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 -1> | 301.3 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 -1> | 301.3 |
AlN (mp-661) | <0 0 1> | <0 1 -1> | 301.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 272.6 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 233.7 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 350.5 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 311.6 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 350.5 |
GaAs (mp-2534) | <1 0 0> | <1 -1 1> | 259.5 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 272.6 |
Te2W (mp-22693) | <1 1 1> | <0 0 1> | 116.8 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 233.7 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 153.0 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 235.5 |
GaN (mp-804) | <1 0 1> | <1 -1 -1> | 253.3 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 116.8 |
GaN (mp-804) | <1 1 1> | <1 0 -1> | 154.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 311.6 |
SiO2 (mp-6930) | <1 0 1> | <1 -1 -1> | 253.3 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 350.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 272.6 |
SiO2 (mp-6930) | <1 1 0> | <0 1 -1> | 241.1 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 155.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 272.6 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 272.6 |
GaSe (mp-1943) | <1 0 0> | <1 -1 1> | 259.5 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 272.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 350.5 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 174.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 -1> | 180.8 |
InAs (mp-20305) | <1 1 1> | <1 -1 1> | 259.5 |
BN (mp-984) | <0 0 1> | <0 0 1> | 194.7 |
BN (mp-984) | <1 0 1> | <1 0 0> | 306.0 |
BN (mp-984) | <1 1 0> | <1 -1 1> | 259.5 |
BN (mp-984) | <1 1 1> | <0 0 1> | 272.6 |
ZnSe (mp-1190) | <1 0 0> | <1 -1 1> | 259.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 -1> | 180.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 350.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 272.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 194.7 |
LiNbO3 (mp-3731) | <1 1 0> | <1 -1 -1> | 253.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 77.9 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 229.5 |
CdS (mp-672) | <1 0 1> | <0 1 -1> | 301.3 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 155.8 |
CdS (mp-672) | <1 1 1> | <0 1 -1> | 301.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 77.9 |
LiF (mp-1138) | <1 0 0> | <0 1 -1> | 180.8 |
LiF (mp-1138) | <1 1 1> | <1 0 -1> | 308.0 |
MoS2 (mp-1434) | <0 0 1> | <1 0 -1> | 231.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Hg3SeO6 (mp-676169) | 0.7177 | 0.559 | 3 |
AlTeI7 (mp-29407) | 0.7314 | 0.000 | 3 |
CrPO4 (mp-540463) | 0.6788 | 0.700 | 3 |
AsWO5 (mvc-5992) | 0.6554 | 0.218 | 3 |
Mn5(P2O7)4 (mp-704209) | 0.7305 | 0.481 | 3 |
Na2PH15O11 (mp-708993) | 0.5021 | 0.019 | 4 |
LiCr2P3O13 (mp-705400) | 0.6228 | 0.163 | 4 |
Na4P4(H2O5)3 (mp-740750) | 0.6149 | 0.032 | 4 |
Fe3P2(H2O3)4 (mp-745134) | 0.5874 | 0.186 | 4 |
NaP(HO2)2 (mp-697367) | 0.5720 | 0.032 | 4 |
Li2NiH12(SO7)2 (mp-771658) | 0.5085 | 0.114 | 5 |
LiMn2P2H5O11 (mp-780864) | 0.4383 | 0.224 | 5 |
Li4MnH6(S2O9)2 (mp-778774) | 0.5252 | 0.057 | 5 |
Li2MnH4(SO5)2 (mp-772273) | 0.4069 | 0.183 | 5 |
Mg2Cu2P2(H4O5)3 (mp-740757) | 0.4297 | 0.021 | 5 |
NaMnP2H10NO10 (mp-761339) | 0.7164 | 0.119 | 6 |
Na4TeMo6H40(NO20)2 (mp-744242) | 0.6418 | 0.517 | 6 |
KNaZrSi3H4O11 (mp-773906) | 0.6180 | 0.000 | 6 |
NaMgH4SO6F (mp-766031) | 0.6938 | 0.007 | 6 |
NaCoBP2H2O9 (mp-601388) | 0.6873 | 0.072 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv H S O |
Final Energy/Atom-5.6421 eV |
Corrected Energy-236.5650 eV
-236.5650 eV = -214.3994 eV (uncorrected energy) - 16.6996 eV (MP Anion Correction) - 5.4660 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)