Final Magnetic Moment0.004 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.888 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.057 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi3SbO4 + LiCoSbO4 + LiSbO3 + Sb2O3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 67.3 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 111.5 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 190.7 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 269.1 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 269.1 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 185.8 |
Te2W (mp-22693) | <1 0 1> | <1 0 0> | 190.7 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 317.8 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 63.6 |
Te2Mo (mp-602) | <1 1 0> | <1 0 1> | 92.9 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 254.2 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 223.0 |
BN (mp-984) | <1 0 0> | <1 0 0> | 317.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 134.5 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 111.5 |
SiC (mp-7631) | <1 0 0> | <1 0 1> | 92.9 |
SiC (mp-7631) | <1 0 1> | <1 0 0> | 190.7 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 269.1 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 317.8 |
TiO2 (mp-2657) | <1 0 0> | <1 0 1> | 278.7 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 201.8 |
TiO2 (mp-2657) | <1 1 1> | <0 1 1> | 260.4 |
C (mp-66) | <1 0 0> | <0 0 1> | 269.1 |
Mg (mp-153) | <0 0 1> | <1 0 1> | 278.7 |
Mg (mp-153) | <1 0 0> | <1 0 1> | 185.8 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 134.5 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 254.2 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 254.2 |
MoSe2 (mp-1634) | <1 0 1> | <0 1 1> | 260.4 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 1> | 185.8 |
Au (mp-81) | <1 1 0> | <0 1 0> | 223.0 |
C (mp-48) | <1 0 0> | <1 0 0> | 190.7 |
C (mp-48) | <1 0 1> | <0 1 1> | 260.4 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 201.8 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 63.6 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 317.8 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 185.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 134.5 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 111.5 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 269.1 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 254.2 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 254.2 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 317.8 |
Te2W (mp-22693) | <1 0 0> | <1 0 1> | 92.9 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 134.5 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 190.7 |
BN (mp-984) | <1 0 1> | <0 1 1> | 260.4 |
BN (mp-984) | <1 1 1> | <1 0 0> | 317.8 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 190.7 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 190.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mg(SnO2)2 (mvc-5221) | 0.3585 | 0.138 | 3 |
Fe2CuO4 (mp-705659) | 0.3684 | 0.589 | 3 |
Mg(MoO2)2 (mvc-6124) | 0.2888 | 0.200 | 3 |
Ca(WO2)2 (mvc-10243) | 0.3345 | 0.458 | 3 |
Ca(WO2)2 (mvc-10486) | 0.3407 | 0.499 | 3 |
Li4Mn5Nb3O16 (mp-773388) | 0.1494 | 0.724 | 4 |
Li4Mn5Sb3O16 (mp-769848) | 0.1913 | 0.112 | 4 |
Li4Mn5V3O16 (mp-773194) | 0.2092 | 0.230 | 4 |
Li4Fe3Sb5O16 (mp-769870) | 0.1476 | 0.046 | 4 |
Li4Ni3Sb5O16 (mp-774248) | 0.0956 | 0.081 | 4 |
Al2Se3 (mp-685120) | 0.5793 | 0.028 | 2 |
Co23O32 (mp-705564) | 0.5819 | 0.093 | 2 |
Si3N4 (mp-641539) | 0.5733 | 0.288 | 2 |
Ge3N4 (mp-641541) | 0.5305 | 0.208 | 2 |
Fe23O32 (mp-776135) | 0.5362 | 0.110 | 2 |
Li4Ti3Fe3(TeO8)2 (mp-762517) | 0.2144 | 0.193 | 5 |
Li4Mn3Cu2Sb3O16 (mp-775072) | 0.1793 | 0.242 | 5 |
Li4Co3Cu3(TeO8)2 (mp-766631) | 0.2102 | 0.022 | 5 |
Li4Co3Cu2Sb3O16 (mp-763275) | 0.1639 | 0.147 | 5 |
Li4Ti3Mn3(CuO8)2 (mp-781494) | 0.1803 | 0.083 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Co Sb O |
Final Energy/Atom-5.8847 eV |
Corrected Energy-363.2602 eV
-363.2602 eV = -329.5429 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction) - 11.2440 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)