Final Magnetic Moment0.110 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.954 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.101 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.64 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2TiO3 + LiCuO2 + CuO |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2 [5] |
HallC 2y |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 323.8 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 71.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 329.7 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 286.7 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 141.3 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 235.5 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 214.9 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 214.9 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 269.9 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 54.0 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 286.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 141.3 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 94.2 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 141.3 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 47.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 94.2 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 215.9 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 54.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 269.9 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 164.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 188.4 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 215.9 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 269.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 161.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 269.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 54.0 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 247.3 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 235.5 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 282.6 |
LiF (mp-1138) | <1 1 1> | <1 1 0> | 295.6 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 247.3 |
Te2W (mp-22693) | <0 1 0> | <0 1 1> | 214.9 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 323.8 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 215.9 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 197.1 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 282.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 141.3 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 247.3 |
Ag (mp-124) | <1 1 1> | <1 1 0> | 295.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 323.8 |
BN (mp-984) | <0 0 1> | <0 0 1> | 329.7 |
BN (mp-984) | <1 0 0> | <0 0 1> | 235.5 |
BN (mp-984) | <1 0 1> | <1 0 1> | 286.7 |
BN (mp-984) | <1 1 0> | <0 0 1> | 329.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 247.3 |
Bi2Se3 (mp-541837) | <1 0 0> | <1 0 0> | 247.3 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 141.3 |
Al (mp-134) | <1 0 0> | <0 1 0> | 161.9 |
Al (mp-134) | <1 1 1> | <0 1 0> | 54.0 |
MoS2 (mp-1434) | <1 1 0> | <0 0 1> | 235.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mg7Cu17O24 (mp-758051) | 0.3682 | 0.057 | 3 |
Mg4Cu11O15 (mp-758194) | 0.3954 | 0.079 | 3 |
Mg2Cu5O7 (mp-757254) | 0.3902 | 0.077 | 3 |
MgCuO2 (mvc-4732) | 0.4322 | 0.084 | 3 |
LiCr3O4 (mp-774235) | 0.2808 | 0.134 | 3 |
Li5Mn2Cu5O12 (mp-764735) | 0.0968 | 0.122 | 4 |
Li5Cr2Cu5O12 (mp-773227) | 0.1281 | 0.088 | 4 |
Li5Cu5(NiO6)2 (mp-773217) | 0.2017 | 0.129 | 4 |
Li5Nb2Cu5O12 (mp-756927) | 0.1440 | 0.115 | 4 |
Li5Cu5(SbO6)2 (mp-756817) | 0.1494 | 0.059 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Ti_pv Cu_pv O |
Final Energy/Atom-5.9861 eV |
Corrected Energy-152.0941 eV
-152.0941 eV = -143.6666 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)