Final Magnetic Moment0.959 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.483 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.084 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.06 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNb2(PO4)3 + PH3O4 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 337.9 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 285.5 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 187.7 |
CdS (mp-672) | <1 0 0> | <1 -1 0> | 198.8 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 228.4 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 150.2 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 252.6 |
YVO4 (mp-19133) | <1 1 1> | <0 1 0> | 84.2 |
Te2Mo (mp-602) | <0 0 1> | <0 1 1> | 285.5 |
Te2Mo (mp-602) | <1 0 0> | <1 -1 0> | 265.0 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 294.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 337.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 187.7 |
Bi2Se3 (mp-541837) | <1 0 0> | <1 1 0> | 248.1 |
Al (mp-134) | <1 0 0> | <1 0 0> | 248.0 |
Al (mp-134) | <1 1 0> | <0 1 0> | 252.6 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 112.6 |
LiGaO2 (mp-5854) | <0 1 1> | <1 1 0> | 82.7 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 168.4 |
LiGaO2 (mp-5854) | <1 0 1> | <1 -1 1> | 307.1 |
TeO2 (mp-2125) | <1 0 0> | <0 1 0> | 210.5 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 337.9 |
SiC (mp-7631) | <1 1 1> | <1 0 0> | 248.0 |
LiTaO3 (mp-3666) | <0 0 1> | <0 1 0> | 294.7 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 126.3 |
MgO (mp-1265) | <1 1 0> | <0 1 1> | 342.6 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 112.6 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 248.0 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 262.8 |
C (mp-66) | <1 0 0> | <0 1 0> | 294.7 |
C (mp-66) | <1 1 0> | <0 0 1> | 225.2 |
C (mp-66) | <1 1 1> | <1 0 1> | 220.9 |
GdScO3 (mp-5690) | <0 0 1> | <1 -1 0> | 66.3 |
GdScO3 (mp-5690) | <0 1 0> | <1 -1 1> | 230.3 |
GdScO3 (mp-5690) | <0 1 1> | <1 1 0> | 165.4 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 0> | 336.8 |
GdScO3 (mp-5690) | <1 0 1> | <1 -1 0> | 331.3 |
GdScO3 (mp-5690) | <1 1 0> | <1 -1 1> | 307.1 |
GdScO3 (mp-5690) | <1 1 1> | <0 1 0> | 294.7 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 210.5 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 112.6 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 294.7 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 112.6 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 187.7 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 248.0 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 112.6 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 126.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 112.6 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 337.9 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 228.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr(PO4)2 (mp-767022) | 0.5520 | 0.299 | 3 |
VPO5 (mp-540277) | 0.4664 | 0.060 | 3 |
Sn3(P2O7)2 (mp-673118) | 0.5381 | 0.065 | 3 |
V3(P3O10)2 (mp-32524) | 0.4986 | 0.027 | 3 |
Fe3(P3O10)2 (mp-31877) | 0.5360 | 0.169 | 3 |
V2P4H3O16 (mp-771427) | 0.1338 | 0.077 | 4 |
LiTi(PO3)4 (mp-758240) | 0.4272 | 0.067 | 4 |
Te2P4H3O16 (mp-755681) | 0.1918 | 0.075 | 4 |
Sb2P4H3O16 (mp-771965) | 0.3515 | 0.083 | 4 |
CsV2P5O16 (mp-541176) | 0.4658 | 0.001 | 4 |
LiVP3HO10 (mp-853251) | 0.5113 | 0.066 | 5 |
LiVP3HO10 (mp-763631) | 0.5050 | 0.080 | 5 |
LiMnP3HO10 (mp-851011) | 0.5364 | 0.176 | 5 |
CsGaP3HO10 (mp-703308) | 0.4467 | 0.000 | 5 |
LiVP3HO10 (mp-774404) | 0.5138 | 0.088 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nb_pv P H O |
Final Energy/Atom-7.2635 eV |
Corrected Energy-192.8240 eV
-192.8240 eV = -181.5873 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)