Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.574 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.263 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.82 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiFe(CO3)2 + LiFeAs2O7 + O2 |
Band Gap0.048 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 244.9 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 70.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 244.9 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 232.2 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 290.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 104.9 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 139.9 |
CeO2 (mp-20194) | <1 0 0> | <1 0 -1> | 329.5 |
CeO2 (mp-20194) | <1 1 1> | <1 0 -1> | 263.6 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 232.2 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 278.0 |
GaN (mp-804) | <0 0 1> | <1 0 -1> | 197.7 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 279.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 314.8 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 149.5 |
GaN (mp-804) | <1 1 1> | <1 1 -1> | 241.7 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 176.0 |
SiO2 (mp-6930) | <1 0 0> | <1 0 -1> | 329.5 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 293.3 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 278.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 209.9 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 211.9 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 -1> | 161.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 1> | 253.4 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 244.9 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 278.0 |
Te2Mo (mp-602) | <1 0 1> | <1 0 -1> | 329.5 |
ZnSe (mp-1190) | <1 0 0> | <0 1 1> | 232.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 349.8 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 174.9 |
GaSe (mp-1943) | <1 1 0> | <1 0 0> | 117.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 314.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 224.3 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 -1> | 329.5 |
CdS (mp-672) | <0 0 1> | <1 1 -1> | 241.7 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 139.9 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 314.8 |
BN (mp-984) | <1 0 1> | <0 1 0> | 139.0 |
BN (mp-984) | <1 1 1> | <1 1 0> | 299.0 |
LiNbO3 (mp-3731) | <1 0 1> | <0 1 1> | 232.2 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 141.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 314.8 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 290.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 -1> | 241.7 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 224.3 |
YVO4 (mp-19133) | <0 0 1> | <1 0 -1> | 329.5 |
TePb (mp-19717) | <1 0 0> | <1 0 -1> | 131.8 |
Al (mp-134) | <1 0 0> | <0 0 1> | 314.8 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 -1> | 329.5 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 -1> | 65.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Bi(BO2)3 (mp-23349) | 0.7211 | 0.001 | 3 |
Bi(BO2)3 (mp-1079609) | 0.7334 | 0.006 | 3 |
CuSeO4 (mp-554040) | 0.7155 | 0.000 | 3 |
Li3Fe(BO2)5 (mp-761304) | 0.5980 | 0.132 | 4 |
Li3V(BO2)5 (mp-770344) | 0.5112 | 0.111 | 4 |
Li3Mn(BO2)5 (mp-771291) | 0.5882 | 0.198 | 4 |
Na3Ca(BO2)5 (mp-614628) | 0.5563 | 0.002 | 4 |
Li3Ni(BO2)5 (mp-771081) | 0.5506 | 0.092 | 4 |
LiMnCSO7 (mp-780035) | 0.3204 | 0.218 | 5 |
LiCoCSO7 (mp-773196) | 0.3737 | 0.129 | 5 |
LiCuCSO7 (mp-768599) | 0.3698 | 0.060 | 5 |
LiFePCO7 (mp-25529) | 0.2514 | 0.235 | 5 |
LiNiPCO7 (mp-25602) | 0.3917 | 0.177 | 5 |
Li12VCr3P4(CO7)4 (mp-767735) | 0.7454 | 0.075 | 6 |
KLiMnPCO7 (mp-764256) | 0.4993 | 0.000 | 6 |
Li6MnNiP2(CO7)2 (mp-767293) | 0.7443 | 0.046 | 6 |
NaLiMnPCO7 (mp-763833) | 0.5312 | 0.062 | 6 |
CdRe2H8C2(N2O5)2 (mp-733848) | 0.6866 | 0.016 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv As C O |
Final Energy/Atom-6.2330 eV |
Corrected Energy-151.2559 eV
Uncorrected energy = -137.1259 eV
Composition-based energy adjustment (-0.687 eV/atom x 14.0 atoms) = -9.6180 eV
Composition-based energy adjustment (-2.256 eV/atom x 2.0 atoms) = -4.5120 eV
Corrected energy = -151.2559 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)