Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.837 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.019 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.20 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBa3GeO5 |
Band Gap2.695 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [160] |
HallR 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 225.3 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 225.3 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 225.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 225.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 169.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 281.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 169.0 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 281.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 169.0 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 225.3 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 56.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 169.0 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 225.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 225.3 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 225.3 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 56.3 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 225.3 |
BN (mp-984) | <1 0 1> | <0 0 1> | 225.3 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 225.3 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 281.7 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 225.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 225.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 169.0 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 169.0 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 169.0 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 225.3 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 169.0 |
Al (mp-134) | <1 1 0> | <0 0 1> | 281.7 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 281.7 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 225.3 |
C (mp-66) | <1 1 0> | <0 0 1> | 281.7 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 169.0 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 225.3 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 225.3 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 225.3 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 225.3 |
InSb (mp-20012) | <1 1 1> | <0 0 1> | 225.3 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 169.0 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 281.7 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 281.7 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 169.0 |
WS2 (mp-224) | <1 0 0> | <0 0 1> | 225.3 |
WS2 (mp-224) | <1 1 0> | <0 0 1> | 225.3 |
WS2 (mp-224) | <1 1 1> | <0 0 1> | 225.3 |
C (mp-48) | <0 0 1> | <0 0 1> | 225.3 |
C (mp-48) | <1 0 1> | <0 0 1> | 338.0 |
NaCl (mp-22862) | <1 1 0> | <0 0 1> | 225.3 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 225.3 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 56.3 |
YAlO3 (mp-3792) | <0 1 1> | <0 0 1> | 338.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca3SiO5 (mp-558273) | 0.2558 | 0.050 | 3 |
Ba2GeO4 (mp-752410) | 0.7296 | 0.050 | 3 |
Ba3GeO5 (mp-756637) | 0.5353 | 0.027 | 3 |
Ca3SiO5 (mp-554141) | 0.6502 | 0.061 | 3 |
Ca3SiO5 (mp-37657) | 0.5317 | 0.029 | 3 |
Na3SO4F (mp-560222) | 0.7178 | 0.000 | 4 |
Na3WO4F (mp-565594) | 0.6270 | 0.004 | 4 |
LiCdPO4 (mp-556786) | 0.7194 | 0.000 | 4 |
CrAg3ClO4 (mp-566124) | 0.6745 | 0.022 | 4 |
LiPWO4 (mp-635084) | 0.7427 | 0.562 | 4 |
Na2CaPO4F (mp-39260) | 0.5485 | 0.027 | 5 |
Na15S5Cl(O5F)4 (mp-554285) | 0.5162 | 0.000 | 5 |
Na2MnPO4F (mp-566286) | 0.6189 | 0.595 | 5 |
Na21S7Cl(O14F3)2 (mp-680169) | 0.5558 | 0.002 | 5 |
Li2VPO4F (mp-849509) | 0.6394 | 0.365 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Ge_d O |
Final Energy/Atom-6.3486 eV |
Corrected Energy-181.7161 eV
Uncorrected energy = -171.4111 eV
Composition-based energy adjustment (-0.687 eV/atom x 15.0 atoms) = -10.3050 eV
Corrected energy = -181.7161 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)