Final Magnetic Moment0.148 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.160 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.259 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.70 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi(NiO2)2 + NiO + Li2SnO3 |
Band Gap0.512 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 178.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 311.6 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 222.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 133.6 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 222.6 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 311.6 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 311.6 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 202.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 257.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 267.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 222.6 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 222.6 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 257.1 |
BaF2 (mp-1029) | <1 0 0> | <1 1 0> | 202.6 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 133.6 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 222.6 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 44.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 257.1 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 261.9 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 133.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 257.1 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 267.1 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 222.6 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 261.9 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 267.1 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 261.9 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 174.6 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 222.6 |
C (mp-66) | <1 0 0> | <0 0 1> | 311.6 |
C (mp-66) | <1 1 0> | <0 0 1> | 89.0 |
GdScO3 (mp-5690) | <0 0 1> | <0 1 0> | 257.1 |
GdScO3 (mp-5690) | <1 1 0> | <0 1 0> | 257.1 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 267.1 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 267.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 311.6 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 133.6 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 154.2 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 222.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 133.6 |
GaSe (mp-1943) | <1 0 0> | <1 0 1> | 198.4 |
GaSe (mp-1943) | <1 0 1> | <0 1 0> | 205.7 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 267.1 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 222.6 |
PbS (mp-21276) | <1 1 0> | <1 0 0> | 261.9 |
BN (mp-984) | <0 0 1> | <1 0 0> | 87.3 |
BN (mp-984) | <1 0 0> | <0 0 1> | 311.6 |
BN (mp-984) | <1 0 1> | <0 1 1> | 204.0 |
BN (mp-984) | <1 1 0> | <0 0 1> | 133.6 |
BN (mp-984) | <1 1 1> | <0 0 1> | 133.6 |
TbScO3 (mp-31119) | <1 1 0> | <0 1 0> | 257.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2Cr3O6 (mp-771534) | 0.3268 | 0.098 | 3 |
Li5Fe5O12 (mp-771687) | 0.1786 | 0.092 | 3 |
Li2Mn3O6 (mp-773276) | 0.3468 | 0.098 | 3 |
Li2(NiO2)3 (mp-773252) | 0.2657 | 0.241 | 3 |
TlIn5S7 (mp-562480) | 0.5144 | 0.000 | 3 |
Li4FeNi5O12 (mp-771577) | 0.2207 | 0.134 | 4 |
Li4Mn5CoO12 (mp-771545) | 0.2250 | 0.086 | 4 |
Li4Ti5VO12 (mp-771445) | 0.2288 | 0.105 | 4 |
Li4Fe5NiO12 (mp-770801) | 0.2017 | 0.106 | 4 |
Li2Fe2SnO6 (mp-771808) | 0.2242 | 0.283 | 4 |
Tl4O3 (mp-27684) | 0.7344 | 0.000 | 2 |
In6Se7 (mp-567596) | 0.5882 | 0.042 | 2 |
In6S7 (mp-555853) | 0.5221 | 0.008 | 2 |
Li4Ti2Mn3(Fe2O9)2 (mp-769444) | 0.5732 | 0.081 | 5 |
Li4Ti4MnCr4O18 (mp-769442) | 0.5772 | 0.092 | 5 |
Li4Ti4V4CoO18 (mp-769478) | 0.5998 | 0.092 | 5 |
Li4Ti4Mn(Fe2O9)2 (mp-769443) | 0.5963 | 0.087 | 5 |
Li4Ti2Fe4(CoO6)3 (mp-776197) | 0.5547 | 0.217 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Ni_pv Sn_d O |
Final Energy/Atom-4.8268 eV |
Corrected Energy-125.4374 eV
-125.4374 eV = -106.1899 eV (uncorrected energy) - 10.8200 eV (MP Advanced Correction) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)