Final Magnetic Moment0.997 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.131 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.041 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.82 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMn(IO3)2 |
Band Gap1.955 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbcn [60] |
Hall-P 2n 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 186.5 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 204.5 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 261.1 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 261.1 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 269.5 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 81.7 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 111.9 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 89.8 |
SiO2 (mp-6930) | <0 0 1> | <1 1 0> | 130.9 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 81.7 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 186.5 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 163.4 |
BaF2 (mp-1029) | <1 1 1> | <1 1 0> | 130.9 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 89.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 335.7 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 111.9 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 149.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 186.5 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 1> | 89.8 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 163.4 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 163.4 |
InAs (mp-20305) | <1 1 1> | <1 1 0> | 130.9 |
ZnSe (mp-1190) | <1 0 0> | <0 1 1> | 269.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 335.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 204.5 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 245.1 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 111.9 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 335.7 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 102.2 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 335.7 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 111.9 |
LiF (mp-1138) | <1 0 0> | <0 1 1> | 269.5 |
LiF (mp-1138) | <1 1 1> | <1 1 0> | 261.8 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 261.1 |
YVO4 (mp-19133) | <0 0 1> | <0 1 1> | 269.5 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 261.1 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 245.1 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 298.4 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 163.4 |
Te2Mo (mp-602) | <1 0 1> | <0 1 1> | 269.5 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 335.7 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 335.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 335.7 |
BN (mp-984) | <0 0 1> | <1 1 0> | 130.9 |
BN (mp-984) | <1 0 0> | <0 1 1> | 269.5 |
BN (mp-984) | <1 0 1> | <0 0 1> | 223.8 |
BN (mp-984) | <1 1 0> | <0 0 1> | 298.4 |
BN (mp-984) | <1 1 1> | <0 0 1> | 335.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 245.1 |
Al (mp-134) | <1 1 0> | <1 0 0> | 204.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ni(IO3)2 (mp-772376) | 0.3568 | 0.046 | 3 |
CuO2F (mp-997107) | 0.4956 | 0.128 | 3 |
Sr(IO3)2 (mp-754869) | 0.4674 | 0.026 | 3 |
Mg(IO3)2 (mp-768315) | 0.1145 | 0.062 | 3 |
Co(IO3)2 (mp-774233) | 0.4082 | 0.145 | 3 |
LiIn(IO3)4 (mp-973966) | 0.4504 | 0.000 | 4 |
Na2W(OF2)2 (mp-541649) | 0.5634 | 0.000 | 4 |
LiVWO6 (mp-768026) | 0.5206 | 0.054 | 4 |
NaFe(WO4)2 (mp-25534) | 0.5765 | 0.156 | 4 |
YMn(WO4)2 (mvc-622) | 0.5607 | 0.049 | 4 |
UO3 (mp-294) | 0.7361 | 0.082 | 2 |
WF4 (mvc-14582) | 0.7380 | 0.060 | 2 |
BiF5 (mvc-3518) | 0.7343 | 0.004 | 2 |
Ni2O5 (mp-1094139) | 0.7020 | 0.533 | 2 |
K2PtN4(ClO4)2 (mp-669540) | 0.7253 | 0.034 | 5 |
Sr2NiSe2(ClO3)2 (mp-566796) | 0.7339 | 0.000 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Mn_pv I O |
Final Energy/Atom-5.1363 eV |
Corrected Energy-208.4848 eV
-208.4848 eV = -184.9065 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)