Final Magnetic Moment2.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.288 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.123 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.03 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFeO + Li3VO4 + V2O3 |
Band Gap0.851 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 209.2 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 251.6 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 122.4 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 296.6 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 197.7 |
GaAs (mp-2534) | <1 0 0> | <1 0 -1> | 98.9 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 174.3 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 139.4 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 313.7 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 234.9 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 234.9 |
GaN (mp-804) | <0 0 1> | <1 0 -1> | 247.1 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 169.6 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 156.6 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 301.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 180.0 |
SiO2 (mp-6930) | <1 1 0> | <1 1 -1> | 141.1 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 254.4 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 139.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 209.2 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 169.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 313.7 |
ZnSe (mp-1190) | <1 0 0> | <1 0 -1> | 98.9 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 174.3 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 313.7 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 139.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 240.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 69.7 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 174.3 |
CdS (mp-672) | <0 0 1> | <1 0 -1> | 247.1 |
CdS (mp-672) | <1 0 0> | <0 1 1> | 234.9 |
LiF (mp-1138) | <1 0 0> | <0 1 1> | 234.9 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 69.7 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 60.0 |
Te2W (mp-22693) | <0 1 0> | <0 1 1> | 156.6 |
Te2W (mp-22693) | <0 1 1> | <1 0 -1> | 296.6 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 201.3 |
YVO4 (mp-19133) | <0 0 1> | <1 1 0> | 306.0 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 174.3 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 313.7 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 34.9 |
Ag (mp-124) | <1 1 0> | <1 0 -1> | 49.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 60.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 120.0 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 180.0 |
BN (mp-984) | <0 0 1> | <1 0 0> | 244.0 |
BN (mp-984) | <1 0 1> | <1 0 0> | 244.0 |
BN (mp-984) | <1 1 0> | <0 0 1> | 240.1 |
BN (mp-984) | <1 0 0> | <1 0 0> | 278.9 |
BN (mp-984) | <1 1 1> | <1 0 -1> | 346.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3(CoO2)4 (mp-764781) | 0.1789 | 0.121 | 3 |
Li4Cr5O10 (mp-763579) | 0.2219 | 0.035 | 3 |
Li3Cr4O8 (mp-771288) | 0.2172 | 0.034 | 3 |
Li3(NiO2)4 (mvc-16810) | 0.1677 | 0.017 | 3 |
Li3(CoO2)4 (mvc-16807) | 0.1768 | 0.178 | 3 |
Li3MnFe3O8 (mp-767659) | 0.1237 | 0.319 | 4 |
Li3Cr3CoO8 (mp-763184) | 0.1057 | 0.248 | 4 |
Li3V3CoO8 (mp-773242) | 0.0571 | 0.139 | 4 |
Li3NbFe3O8 (mp-763729) | 0.1024 | 0.472 | 4 |
Li3VFe3O8 (mp-762710) | 0.1361 | 0.474 | 4 |
Fe8O9 (mp-763787) | 0.2310 | 0.063 | 2 |
Fe9O10 (mp-763441) | 0.2411 | 0.350 | 2 |
Fe7O8 (mp-715333) | 0.1828 | 0.064 | 2 |
Fe8O9 (mp-705588) | 0.2393 | 0.050 | 2 |
Fe10O11 (mp-705555) | 0.2558 | 0.046 | 2 |
Li6Mn3Cr2Fe3O16 (mp-861553) | 0.4461 | 0.882 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eVFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv V_pv Fe_pv O |
Final Energy/Atom-6.7962 eV |
Corrected Energy-115.3409 eV
-115.3409 eV = -101.9436 eV (uncorrected energy) - 7.7790 eV (MP Advanced Correction) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)