Final Magnetic Moment6.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.553 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.010 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.06 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi19Ni23O42 + NiO + Li2MnO3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 1 0> | 244.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 275.9 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 34.5 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 48.9 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 172.4 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 310.4 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 244.7 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 231.9 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 168.9 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 231.9 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 154.6 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 342.6 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 293.6 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 195.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 179.5 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 146.8 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 172.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 97.9 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 137.9 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 168.9 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 310.4 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 310.4 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 34.5 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 48.9 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 172.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 1> | 97.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 69.0 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 172.4 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 179.5 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 241.4 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 172.4 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 342.6 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 34.5 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 48.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 59.8 |
BN (mp-984) | <1 0 1> | <0 1 0> | 244.7 |
BN (mp-984) | <1 1 0> | <0 1 0> | 342.6 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 195.8 |
Te2W (mp-22693) | <0 1 0> | <0 1 1> | 154.6 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 293.6 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 299.2 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 275.9 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 244.7 |
Al (mp-134) | <1 0 0> | <0 1 1> | 231.9 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 172.4 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 137.9 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 172.4 |
CdTe (mp-406) | <1 1 0> | <1 1 1> | 195.2 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 97.9 |
TeO2 (mp-2125) | <1 0 0> | <0 1 0> | 146.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3Co11O14 (mp-761816) | 0.1748 | 0.285 | 3 |
Li5Fe7O12 (mp-771531) | 0.1706 | 0.025 | 3 |
Li3Co13O16 (mp-868302) | 0.1343 | 0.099 | 3 |
Li5Fe11O16 (mp-768075) | 0.1433 | 0.020 | 3 |
LiCoO2 (mp-1097885) | 0.1675 | 0.043 | 3 |
Li3Mn(CoO2)4 (mp-770976) | 0.1188 | 0.059 | 4 |
Li3TiV4O8 (mp-775104) | 0.0719 | 0.059 | 4 |
Li3Ti(NiO2)4 (mp-771100) | 0.0907 | 0.024 | 4 |
Li3Ti(CoO2)4 (mp-771086) | 0.0778 | 0.065 | 4 |
Li3Ni4SbO8 (mp-774126) | 0.0944 | 0.021 | 4 |
LiTe3 (mp-27466) | 0.2335 | 0.009 | 2 |
Bi2Te3 (mp-568390) | 0.3362 | 0.248 | 2 |
In2Se3 (mp-1068548) | 0.2797 | 0.530 | 2 |
In2Se3 (mp-20830) | 0.2918 | 0.530 | 2 |
Sb2Te3 (mp-1080789) | 0.2560 | 0.129 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.5870 | 0.005 | 5 |
Hg (mp-982872) | 0.4134 | 0.020 | 1 |
Sb (mp-632286) | 0.4601 | 0.059 | 1 |
Se (mp-7755) | 0.4575 | 0.181 | 1 |
Te (mp-10654) | 0.4544 | 0.047 | 1 |
Te (mp-105) | 0.3521 | 0.047 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Ni_pv O |
Final Energy/Atom-5.4057 eV |
Corrected Energy-102.4463 eV
-102.4463 eV = -86.4912 eV (uncorrected energy) - 10.3369 eV (MP Advanced Correction) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)