Final Magnetic Moment1.885 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.085 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.057 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.08 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNaCuO2 + Na2CO3 + SiO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 250.2 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 119.1 |
AlN (mp-661) | <1 0 1> | <1 1 1> | 250.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 168.7 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 337.3 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 173.3 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 173.3 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 337.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 33.7 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 234.5 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 227.4 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 178.7 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 236.1 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 57.8 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 250.2 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 288.8 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 288.8 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 57.8 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 328.2 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 168.7 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 59.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 1> | 250.2 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 1> | 250.2 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 234.5 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 275.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 303.6 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 288.8 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 303.6 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 269.9 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 328.2 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 303.6 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 227.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 337.3 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 328.2 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 269.9 |
YVO4 (mp-19133) | <1 0 0> | <1 0 1> | 138.0 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 67.5 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 168.7 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 59.6 |
TePb (mp-19717) | <1 1 1> | <1 0 0> | 297.9 |
Te2Mo (mp-602) | <0 0 1> | <0 1 1> | 173.3 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 328.2 |
Te2Mo (mp-602) | <1 0 1> | <1 1 1> | 166.8 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 275.9 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 269.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 101.2 |
GaSe (mp-1943) | <1 1 0> | <1 0 0> | 119.1 |
BN (mp-984) | <1 0 1> | <0 0 1> | 168.7 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 1> | 288.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 303.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na3Ca(BO2)5 (mp-542719) | 0.7449 | 0.000 | 4 |
LiSn10(PO4)7 (mp-765193) | 0.7479 | 0.086 | 4 |
Na3ZnPCO7 (mp-767545) | 0.1939 | 0.002 | 5 |
Na3FeSiCO7 (mp-771513) | 0.1558 | 0.000 | 5 |
Na3FeAsCO7 (mp-771494) | 0.1814 | 0.000 | 5 |
Na3VSiCO7 (mp-771420) | 0.1612 | 0.000 | 5 |
Na3CoAsCO7 (mp-773177) | 0.1992 | 0.000 | 5 |
Na2LiFePCO7 (mp-773678) | 0.2171 | 0.132 | 6 |
Na5LiFe2P2(CO7)2 (mp-773529) | 0.2176 | 0.157 | 6 |
Na5LiFe2P2(CO7)2 (mp-773523) | 0.2014 | 0.148 | 6 |
Na5LiFe2P2(CO7)2 (mp-773446) | 0.2158 | 0.188 | 6 |
Na5LiFe2P2(CO7)2 (mp-773414) | 0.2179 | 0.127 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Cu_pv Si C O |
Final Energy/Atom-6.1158 eV |
Corrected Energy-168.6289 eV
Uncorrected energy = -159.0109 eV
Composition-based energy adjustment (-0.687 eV/atom x 14.0 atoms) = -9.6180 eV
Corrected energy = -168.6289 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)