Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.155 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.017 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.72 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnO + Li2SnO3 + LiMnO2 |
Band Gap0.956 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 -1> | 125.9 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 140.9 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 225.5 |
AlN (mp-661) | <0 0 1> | <0 1 -1> | 42.0 |
AlN (mp-661) | <1 0 0> | <1 -1 1> | 112.4 |
AlN (mp-661) | <1 1 0> | <1 -1 -1> | 239.0 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 305.3 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 298.2 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 169.2 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 170.4 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 338.3 |
GaAs (mp-2534) | <1 1 1> | <0 1 0> | 170.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 366.4 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 292.6 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 140.9 |
BaF2 (mp-1029) | <1 1 0> | <0 1 -1> | 167.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 1> | 248.1 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 253.7 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 -1> | 125.9 |
GaN (mp-804) | <0 0 1> | <1 -1 0> | 152.1 |
GaN (mp-804) | <1 0 0> | <0 1 -1> | 83.9 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 213.0 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 170.4 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 338.3 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 170.4 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 253.7 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 298.2 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 248.1 |
CdS (mp-672) | <0 0 1> | <1 0 -1> | 218.0 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 334.4 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 253.7 |
SiO2 (mp-6930) | <1 0 1> | <1 1 -1> | 310.7 |
SiO2 (mp-6930) | <1 1 1> | <1 0 -1> | 261.7 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 174.4 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 298.2 |
Te2W (mp-22693) | <0 1 0> | <0 1 -1> | 167.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 -1 0> | 304.1 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 213.0 |
YVO4 (mp-19133) | <0 0 1> | <0 1 -1> | 251.8 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 253.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 127.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 213.0 |
Te2Mo (mp-602) | <0 0 1> | <0 1 -1> | 167.9 |
Te2Mo (mp-602) | <1 0 0> | <0 1 -1> | 167.9 |
Te2Mo (mp-602) | <1 0 1> | <0 1 -1> | 167.9 |
Te2Mo (mp-602) | <1 1 1> | <1 -1 -1> | 298.8 |
CdS (mp-672) | <1 1 0> | <1 1 -1> | 310.7 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 213.0 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 140.9 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 140.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li5Ni7O12 (mp-771626) | 0.2101 | 0.015 | 3 |
Li7Fe5O12 (mp-771617) | 0.1752 | 0.016 | 3 |
Li2TiO3 (mp-760017) | 0.1902 | 0.156 | 3 |
Li7V5O12 (mp-776654) | 0.1590 | 0.035 | 3 |
Li7Ni5O12 (mp-771927) | 0.2184 | 0.036 | 3 |
Li5Ni3(SnO5)2 (mp-771450) | 0.1680 | 0.012 | 4 |
Li5Fe3(SnO5)2 (mp-769826) | 0.1695 | 0.019 | 4 |
Li4MnO2F3 (mp-766927) | 0.1561 | 0.080 | 4 |
Li5Mn5V2O12 (mp-769823) | 0.1571 | 0.067 | 4 |
Li5Co3(SnO5)2 (mp-771198) | 0.1677 | 0.061 | 4 |
Te2Au (mp-1662) | 0.4804 | 0.018 | 2 |
NaTe3 (mp-28478) | 0.3074 | 0.000 | 2 |
LiTe3 (mp-27466) | 0.4472 | 0.009 | 2 |
BaO (mp-776658) | 0.5418 | 0.019 | 2 |
Te2Au (mp-567525) | 0.4537 | 0.018 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.4745 | 0.005 | 5 |
Sb (mp-632286) | 0.6436 | 0.059 | 1 |
Bi (mp-567379) | 0.7355 | 0.062 | 1 |
Bi (mp-23152) | 0.7416 | 0.000 | 1 |
Te (mp-570459) | 0.6085 | 0.044 | 1 |
Te (mp-105) | 0.7096 | 0.047 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Sn_d O |
Final Energy/Atom-6.2784 eV |
Corrected Energy-275.2668 eV
-275.2668 eV = -251.1359 eV (uncorrected energy) - 14.0458 eV (MP Anion Correction) - 10.0851 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)