Final Magnetic Moment10.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.052 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.062 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.57 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi4Mn5O12 + LiNb3O8 + LiNbO3 + CuO |
Band Gap0.246 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <0 0 1> | <1 0 0> | 290.4 |
GaN (mp-804) | <1 0 0> | <1 -1 0> | 117.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 245.2 |
GaN (mp-804) | <1 1 0> | <0 1 -1> | 256.4 |
GaN (mp-804) | <1 1 1> | <1 -1 -1> | 268.6 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 -1> | 326.0 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 173.1 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 275.9 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 199.7 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 210.7 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 173.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 122.6 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 214.6 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 245.2 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 264.6 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 173.1 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 288.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 288.6 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 326.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 230.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 57.7 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 183.9 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 173.1 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 288.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 245.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 306.5 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 198.5 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 195.6 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 290.4 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 290.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 153.3 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 266.3 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 57.7 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 337.2 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 275.9 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 153.3 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 288.6 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 275.9 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 92.0 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 153.3 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 122.6 |
Ag (mp-124) | <1 1 1> | <0 1 1> | 332.8 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 230.9 |
SiC (mp-7631) | <0 0 1> | <1 0 -1> | 326.0 |
LiTaO3 (mp-3666) | <0 0 1> | <0 1 -1> | 256.4 |
MgO (mp-1265) | <1 1 1> | <0 1 1> | 332.8 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 337.2 |
C (mp-66) | <1 1 0> | <1 -1 1> | 197.0 |
GdScO3 (mp-5690) | <0 0 1> | <0 1 0> | 230.9 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 -1> | 326.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Zn(SnO2)2 (mvc-5313) | 0.3431 | 0.134 | 3 |
Mg(SnO2)2 (mvc-5221) | 0.3114 | 0.138 | 3 |
Ca(CoO2)2 (mvc-5217) | 0.3401 | 0.282 | 3 |
Ca(WO2)2 (mvc-10486) | 0.3369 | 0.499 | 3 |
Mg(SnO2)2 (mvc-9750) | 0.3386 | 0.242 | 3 |
Li2TiMn3O8 (mp-771575) | 0.2762 | 0.112 | 4 |
Li2Co3WO8 (mp-775180) | 0.2596 | 0.115 | 4 |
Li4Mn5V3O16 (mp-773194) | 0.2646 | 0.230 | 4 |
Li4Ti5Co3O16 (mp-777046) | 0.2707 | 0.109 | 4 |
Li4Co5Te3O16 (mp-781593) | 0.2751 | 0.101 | 4 |
Fe3O4 (mp-715491) | 0.6018 | 0.017 | 2 |
Si3N4 (mp-641539) | 0.5088 | 0.288 | 2 |
Ge3N4 (mp-641541) | 0.4743 | 0.208 | 2 |
Cr3N4 (mp-1014358) | 0.5915 | 0.227 | 2 |
Fe3O4 (mp-650112) | 0.5688 | 0.060 | 2 |
Li4Cr3Cu3(WO8)2 (mp-775703) | 0.2034 | 0.049 | 5 |
Li4V3Cu3(SbO8)2 (mp-771539) | 0.1901 | 0.078 | 5 |
Li4Mn3Cu3(WO8)2 (mp-853212) | 0.1809 | 0.265 | 5 |
Li4Fe3Cu3(WO8)2 (mp-765805) | 0.1943 | 0.058 | 5 |
Li4Co3Cu3(WO8)2 (mp-763112) | 0.1552 | 0.068 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Nb_pv Cu_pv O |
Final Energy/Atom-6.7135 eV |
Corrected Energy-204.2564 eV
-204.2564 eV = -187.9772 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 5.0426 eV (MP Advanced Correction)
|