Final Magnetic Moment7.009 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.836 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.068 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.17 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi4Mn5O12 + MnO2 + Li2TeO4 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP2 [3] |
HallP 2y |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 126.3 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 290.6 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 1> | 232.4 |
LaAlO3 (mp-2920) | <1 1 1> | <1 1 1> | 126.3 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 47.5 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 173.2 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 232.4 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 202.6 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 272.1 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 338.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 81.1 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 332.1 |
KCl (mp-23193) | <1 0 0> | <1 1 1> | 315.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 321.6 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 1> | 315.8 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 1> | 284.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 202.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 121.6 |
CdS (mp-672) | <1 1 1> | <1 1 1> | 252.6 |
LiF (mp-1138) | <1 1 0> | <1 1 1> | 189.5 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 148.4 |
Te2W (mp-22693) | <1 1 0> | <0 1 0> | 222.6 |
YVO4 (mp-19133) | <0 0 1> | <1 1 1> | 252.6 |
YVO4 (mp-19133) | <1 1 1> | <0 1 0> | 247.4 |
Te2Mo (mp-602) | <0 0 1> | <1 0 1> | 174.3 |
Te2Mo (mp-602) | <1 0 0> | <1 1 1> | 315.8 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 321.6 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 283.7 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 148.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 272.1 |
GaSe (mp-1943) | <0 0 1> | <1 1 0> | 193.3 |
BN (mp-984) | <0 0 1> | <0 1 0> | 173.2 |
BN (mp-984) | <1 1 1> | <0 0 1> | 243.2 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 346.3 |
MoS2 (mp-1434) | <1 1 0> | <0 1 1> | 237.4 |
Al (mp-134) | <1 1 1> | <0 1 0> | 148.4 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 41.5 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 324.2 |
CdTe (mp-406) | <1 0 0> | <0 1 0> | 222.6 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 321.6 |
TeO2 (mp-2125) | <0 1 1> | <1 0 0> | 290.6 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 202.6 |
TeO2 (mp-2125) | <1 1 1> | <1 0 0> | 207.5 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 126.3 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 124.5 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 81.1 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 237.4 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 338.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 202.6 |
BaF2 (mp-1029) | <1 0 0> | <1 1 1> | 315.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiFeO3 (mp-771612) | 0.1957 | 0.142 | 3 |
LiSbO3 (mp-4995) | 0.1634 | 0.000 | 3 |
LiVF3 (mp-777894) | 0.3168 | 0.028 | 3 |
Li3Fe5O12 (mp-773247) | 0.3371 | 0.141 | 3 |
Mn3TeO6 (mp-770690) | 0.3230 | 0.027 | 3 |
Li2SnTeO6 (mp-8673) | 0.1928 | 0.000 | 4 |
Li2TiTeO6 (mp-756117) | 0.2480 | 0.000 | 4 |
Li4Fe3TeO12 (mp-772725) | 0.1345 | 0.112 | 4 |
Li4Cr(WO4)3 (mp-776187) | 0.2924 | 0.180 | 4 |
Li4Nb(FeO4)3 (mp-774238) | 0.1919 | 0.139 | 4 |
Fe2O3 (mp-777192) | 0.4705 | 0.732 | 2 |
Mn2O3 (mp-565203) | 0.4287 | 0.000 | 2 |
Mn2O3 (mp-542877) | 0.4668 | 0.007 | 2 |
Mn2O3 (mp-562091) | 0.4755 | 0.007 | 2 |
Cu2O3 (mp-771359) | 0.4496 | 0.000 | 2 |
Li4CrBi(TeO6)2 (mp-775998) | 0.4405 | 0.076 | 5 |
Li4Fe2TeWO12 (mp-768021) | 0.3080 | 0.083 | 5 |
Li4Cr2TeWO12 (mp-775566) | 0.3921 | 0.080 | 5 |
Li4Mn2TeWO12 (mp-768044) | 0.3725 | 0.056 | 5 |
Li4V2CrTeO12 (mp-775632) | 0.4278 | 0.104 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Te O |
Final Energy/Atom-6.0444 eV |
Corrected Energy-134.3572 eV
-134.3572 eV = -120.8872 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction) - 5.0426 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)