Final Magnetic Moment0.113 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.897 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.196 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.87 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNiTeO4 + Ni3TeO6 + TiO2 + O2 |
Band Gap0.284 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 109.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 122.8 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 166.1 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 245.6 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 287.7 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 245.6 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 327.4 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 163.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 163.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 184.2 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 166.1 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 245.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 163.7 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 272.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 245.6 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 166.1 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 272.8 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 122.8 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 61.4 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 307.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 122.8 |
BN (mp-984) | <1 0 0> | <1 0 0> | 327.4 |
BN (mp-984) | <1 1 0> | <0 0 1> | 245.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 184.2 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 307.0 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 1> | 249.2 |
LiNbO3 (mp-3731) | <1 1 1> | <1 0 0> | 272.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 272.8 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 327.4 |
Al (mp-134) | <1 0 0> | <1 0 0> | 163.7 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 163.7 |
TeO2 (mp-2125) | <0 1 0> | <0 1 0> | 287.7 |
TeO2 (mp-2125) | <1 0 0> | <1 0 0> | 218.3 |
TeO2 (mp-2125) | <1 0 1> | <1 0 0> | 163.7 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 272.8 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 184.2 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 307.0 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 1> | 249.2 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 218.3 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 122.8 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 184.2 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 272.8 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 61.4 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 54.6 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 327.4 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 272.8 |
C (mp-66) | <1 0 0> | <0 0 1> | 307.0 |
C (mp-66) | <1 1 0> | <0 0 1> | 184.2 |
C (mp-66) | <1 1 1> | <0 1 0> | 287.7 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 163.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn5Cr3O16 (mp-771553) | 0.2785 | 0.054 | 3 |
NbV3O8 (mp-771572) | 0.2718 | 0.302 | 3 |
MnCr3O8 (mp-764180) | 0.2642 | 0.091 | 3 |
Cr3SbO8 (mp-773170) | 0.2727 | 0.114 | 3 |
Cr3Co5O16 (mp-771924) | 0.2510 | 0.096 | 3 |
Ti3Cu3(TeO8)2 (mp-760579) | 0.1146 | 0.087 | 4 |
Ti3Co3(TeO8)2 (mp-761356) | 0.1868 | 0.101 | 4 |
Co3Ni3(TeO8)2 (mp-851314) | 0.1951 | 0.089 | 4 |
Cr3Co3(SbO8)2 (mp-761807) | 0.2071 | 0.130 | 4 |
Mn3Ni3(TeO8)2 (mp-771860) | 0.1547 | 0.077 | 4 |
TiO2 (mp-775938) | 0.4087 | 0.039 | 2 |
MnO2 (mp-773240) | 0.4078 | 0.030 | 2 |
VO2 (mp-715553) | 0.2963 | 0.273 | 2 |
TiO2 (mp-756587) | 0.3774 | 0.112 | 2 |
CoO2 (mp-769849) | 0.3983 | 0.068 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Ti_pv Ni_pv Te O |
Final Energy/Atom-6.4278 eV |
Corrected Energy-172.8820 eV
Uncorrected energy = -154.2670 eV
Composition-based energy adjustment (-0.687 eV/atom x 16.0 atoms) = -10.9920 eV
Composition-based energy adjustment (-2.541 eV/atom x 3.0 atoms) = -7.6230 eV
Corrected energy = -172.8820 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)