material

NbCrO4

ID:

mp-771686

DOI:

10.17188/1300766


Material Details

Final Magnetic Moment
3.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-2.719 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.062 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.59 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Cr2O3 + Nb2O5
Band Gap
1.040 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4m2 [119]
Hall
I 4 2
Point Group
42m
Crystal System
tetragonal

Electronic Structure

Band Structure
Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
YAlO3 (mp-3792) <1 0 0> <1 1 1> 0.005 281.7
SiC (mp-7631) <0 0 1> <1 1 0> 0.011 108.3
YAlO3 (mp-3792) <0 1 1> <1 0 1> 0.013 289.4
SiC (mp-11714) <0 0 1> <1 1 0> 0.014 108.3
SrTiO3 (mp-4651) <1 1 0> <0 0 1> 0.021 62.5
SrTiO3 (mp-4651) <1 0 1> <1 1 0> 0.023 54.1
CdWO4 (mp-19387) <1 1 1> <1 0 1> 0.032 206.7
GaN (mp-804) <0 0 1> <1 1 0> 0.033 54.1
PbSe (mp-2201) <1 0 0> <0 0 1> 0.045 78.1
C (mp-48) <1 1 1> <1 0 0> 0.046 306.2
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.053 31.2
TiO2 (mp-2657) <1 1 1> <0 0 1> 0.053 234.3
CdS (mp-672) <0 0 1> <1 1 0> 0.057 108.3
LiAlO2 (mp-3427) <1 1 0> <1 1 0> 0.070 324.8
GaN (mp-804) <1 0 0> <1 0 0> 0.075 153.1
LiTaO3 (mp-3666) <1 0 0> <1 0 1> 0.076 289.4
Ni (mp-23) <1 1 0> <1 0 1> 0.076 206.7
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.079 171.8
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.079 171.8
GaSb (mp-1156) <1 0 0> <0 0 1> 0.082 78.1
TeO2 (mp-2125) <0 1 1> <1 1 1> 0.083 225.4
InP (mp-20351) <1 0 0> <0 0 1> 0.085 140.6
Au (mp-81) <1 0 0> <0 0 1> 0.087 140.6
NdGaO3 (mp-3196) <1 0 0> <1 1 0> 0.090 216.5
Y3Fe5O12 (mp-19648) <1 0 0> <0 0 1> 0.091 156.2
CsI (mp-614603) <1 1 1> <1 1 0> 0.094 108.3
SiO2 (mp-6930) <0 0 1> <1 1 1> 0.097 281.7
Te2W (mp-22693) <0 0 1> <1 0 0> 0.106 268.0
BaF2 (mp-1029) <1 0 0> <0 0 1> 0.110 78.1
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.112 281.1
CsI (mp-614603) <1 0 0> <0 0 1> 0.117 62.5
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.120 187.4
CdSe (mp-2691) <1 0 0> <0 0 1> 0.120 78.1
Al2O3 (mp-1143) <1 0 1> <1 0 0> 0.121 268.0
SiO2 (mp-6930) <1 0 0> <0 0 1> 0.124 249.9
Te2Mo (mp-602) <1 1 0> <1 0 0> 0.126 191.4
SiC (mp-11714) <1 0 1> <1 0 1> 0.142 289.4
BN (mp-984) <1 0 1> <0 0 1> 0.142 203.0
ZrO2 (mp-2858) <1 0 -1> <1 0 1> 0.144 289.4
Al2O3 (mp-1143) <0 0 1> <1 1 0> 0.151 162.4
KCl (mp-23193) <1 1 0> <1 0 1> 0.152 289.4
CaF2 (mp-2741) <1 1 0> <1 1 0> 0.152 216.5
NdGaO3 (mp-3196) <1 0 1> <1 1 0> 0.175 54.1
Bi2Se3 (mp-541837) <0 0 1> <1 1 0> 0.179 108.3
DyScO3 (mp-31120) <1 1 0> <0 0 1> 0.197 62.5
TbScO3 (mp-31119) <1 0 0> <1 0 0> 0.198 229.7
GaP (mp-2490) <1 1 0> <1 1 0> 0.199 216.5
Ag (mp-124) <1 0 0> <0 0 1> 0.201 140.6
TeO2 (mp-2125) <0 1 0> <1 1 0> 0.203 270.7
Ni (mp-23) <1 0 0> <0 0 1> 0.208 62.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
382 82 100 0 0 0
82 382 100 0 0 0
100 100 208 0 0 0
0 0 0 36 0 0
0 0 0 0 36 0
0 0 0 0 0 46
Compliance Tensor Sij (10-12Pa-1)
3 -0.3 -1.3 0 0 0
-0.3 3 -1.3 0 0 0
-1.3 -1.3 6.1 0 0 0
0 0 0 28.1 0 0
0 0 0 0 28.1 0
0 0 0 0 0 21.8
Shear Modulus GV
69 GPa
Bulk Modulus KV
171 GPa
Shear Modulus GR
51 GPa
Bulk Modulus KR
159 GPa
Shear Modulus GVRH
60 GPa
Bulk Modulus KVRH
165 GPa
Elastic Anisotropy
1.87
Poisson's Ratio
0.34

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 0.00000 0.00000 0.00000
0.00000 0.00000 0.00000 0.00000 0.00000 0.00000
0.89037 -0.89037 0.00000 0.00000 0.00000 0.00000
Piezoelectric Modulus ‖eijmax
1.25918 C/m2
Crystallographic Direction vmax
0.00000
-1.00000
0.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
6.29 0.00 0.00
0.00 6.29 0.00
0.00 0.00 5.75
Dielectric Tensor εij (total)
96.26 0.00 0.00
0.00 96.26 0.00
0.00 0.00 12.47
Polycrystalline dielectric constant εpoly
(electronic contribution)
6.11
Polycrystalline dielectric constant εpoly
(total)
68.33
Refractive Index n
2.47
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TiNbO4 (mp-755302) 0.0873 0.059 3
TiFeO4 (mp-773534) 0.0756 0.088 3
CoSbO4 (mp-774401) 0.1255 0.122 3
CrSbO4 (mp-774153) 0.0570 0.067 3
MnSbO4 (mp-774143) 0.0857 0.042 3
LiFe5(OF2)4 (mp-782691) 0.4178 0.069 4
Ti2Mn3Cr3O16 (mp-771540) 0.5419 0.083 4
Ti3Mn3Cr2O16 (mp-770915) 0.5605 0.099 4
Mn3Cr3(WO8)2 (mp-778921) 0.5513 0.084 4
LiV(OF)2 (mp-764229) 0.5407 0.027 4
FeO2 (mp-715178) 0.0427 0.145 2
IrO2 (mp-1014261) 0.0773 0.258 2
TiO2 (mp-390) 0.1920 0.006 2
CeSe2 (mp-1080295) 0.0380 0.120 2
TiO2 (mp-34688) 0.1415 0.008 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
Cr: 3.7 eV
Pseudopotentials
VASP PAW: Nb_pv Cr_pv O
Final Energy/Atom
-8.4973 eV
Corrected Energy
-55.8057 eV
-55.8057 eV = -50.9836 eV (uncorrected energy) - 2.8092 eV (MP Anion Correction) - 2.0130 eV (MP Advanced Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)