Final Magnetic Moment9.949 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.375 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.109 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.52 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiCuO2 + Fe2O3 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [166] |
Hall-R 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 207.5 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 237.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 326.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 237.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 266.8 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 207.5 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 237.2 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 207.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 118.6 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 171.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 88.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 326.1 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 207.5 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 257.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 237.2 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 171.8 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 207.5 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 237.2 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 237.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 148.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 118.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 29.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 207.5 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 355.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 148.2 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 118.6 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 29.6 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 266.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 207.5 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 266.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 326.1 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 118.6 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 29.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 118.6 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 88.9 |
BN (mp-984) | <0 0 1> | <0 0 1> | 266.8 |
BN (mp-984) | <1 0 1> | <0 0 1> | 326.1 |
BN (mp-984) | <1 1 0> | <0 0 1> | 266.8 |
BN (mp-984) | <1 1 1> | <1 0 1> | 272.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 207.5 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 266.8 |
Al (mp-134) | <1 0 0> | <0 0 1> | 148.2 |
Al (mp-134) | <1 1 0> | <0 0 1> | 118.6 |
Al (mp-134) | <1 1 1> | <0 0 1> | 29.6 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 266.8 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 237.2 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 177.9 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 266.8 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 207.5 |
C (mp-66) | <1 1 1> | <0 0 1> | 88.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3Ti4O8 (mp-752879) | 0.1599 | 0.045 | 3 |
Li3(CoO2)4 (mp-763750) | 0.2057 | 0.157 | 3 |
Li3Cr4O8 (mp-771288) | 0.1586 | 0.034 | 3 |
Li3(CoO2)4 (mvc-16807) | 0.1489 | 0.196 | 3 |
Li3(FeO2)4 (mp-769726) | 0.1356 | 0.034 | 3 |
Li3TiV3O8 (mp-770960) | 0.0612 | 0.028 | 4 |
Li3TiFe3O8 (mp-769966) | 0.0629 | 0.055 | 4 |
Li3MnV3O8 (mp-764279) | 0.0979 | 0.071 | 4 |
Li3MnCu3O8 (mp-780643) | 0.0973 | 0.072 | 4 |
Li3TiCr3O8 (mp-770070) | 0.0888 | 0.039 | 4 |
Fe7O8 (mp-705548) | 0.2548 | 0.099 | 2 |
V8C7 (mp-542730) | 0.2488 | 0.007 | 2 |
Fe7O8 (mp-32939) | 0.2128 | 0.099 | 2 |
Fe7O8 (mp-715333) | 0.2310 | 0.064 | 2 |
Ni9O10 (mp-656884) | 0.2634 | 0.047 | 2 |
Li6Mn3Cr2Fe3O16 (mp-861553) | 0.5429 | 0.882 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv Cu_pv O |
Final Energy/Atom-5.2237 eV |
Corrected Energy-86.7063 eV
-86.7063 eV = -78.3550 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction) - 2.7330 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)