Final Magnetic Moment11.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.842 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.010 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.32 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiNiO2 + LiFeO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <1 0 1> | 228.1 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 138.1 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 301.8 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 224.4 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 276.1 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 172.6 |
BaF2 (mp-1029) | <1 1 1> | <1 0 1> | 136.9 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 228.1 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 207.1 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 207.1 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 155.3 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 310.7 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 293.4 |
CeO2 (mp-20194) | <1 1 1> | <1 0 1> | 319.3 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 34.5 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 189.9 |
SiO2 (mp-6930) | <0 0 1> | <1 0 -1> | 344.9 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 301.8 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 155.3 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 273.7 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 224.4 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 241.6 |
SiO2 (mp-6930) | <1 1 0> | <1 0 -1> | 344.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 155.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 69.0 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 207.1 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 86.3 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 155.3 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 327.9 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 189.9 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 293.4 |
CdS (mp-672) | <1 1 1> | <1 1 1> | 264.5 |
LiF (mp-1138) | <1 0 0> | <1 0 -1> | 153.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 189.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 362.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 327.9 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 138.1 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 172.6 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 120.8 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 120.8 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 310.7 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 155.3 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 273.7 |
InAs (mp-20305) | <1 1 1> | <1 0 1> | 136.9 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 34.5 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 189.9 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 172.6 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 327.9 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 273.7 |
Te2W (mp-22693) | <1 1 0> | <1 0 1> | 228.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2Ni5O7 (mp-767264) | 0.1553 | 0.017 | 3 |
Li2RhO3 (mp-754870) | 0.1519 | 0.000 | 3 |
Li2BiO3 (mp-769002) | 0.1556 | 0.032 | 3 |
Li2PtO3 (mp-531826) | 0.1477 | 0.000 | 3 |
LiCoO2 (mp-894498) | 0.1296 | 0.032 | 3 |
Li2VFeO4 (mp-770982) | 0.1049 | 0.044 | 4 |
Li2VO2F (mp-780295) | 0.1082 | 0.050 | 4 |
Li2VCrO4 (mp-763906) | 0.1033 | 0.023 | 4 |
Li3Fe(NiO3)2 (mp-773709) | 0.1019 | 0.013 | 4 |
Li3V2FeO6 (mp-771840) | 0.0962 | 0.014 | 4 |
Bi2Te3 (mp-568390) | 0.2255 | 0.248 | 2 |
RbN (mp-1066707) | 0.2684 | 1.513 | 2 |
In2Se3 (mp-20830) | 0.2572 | 0.530 | 2 |
SrN (mp-1078609) | 0.2606 | 0.438 | 2 |
Sb2Te3 (mp-1080789) | 0.2290 | 0.128 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.6363 | 0.005 | 5 |
Hg (mp-982872) | 0.3251 | 0.020 | 1 |
Sb (mp-632286) | 0.3875 | 0.059 | 1 |
Se (mp-7755) | 0.3917 | 0.181 | 1 |
Te (mp-10654) | 0.3449 | 0.047 | 1 |
Te (mp-105) | 0.2956 | 0.047 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eVNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv Ni_pv O |
Final Energy/Atom-5.6994 eV |
Corrected Energy-80.2367 eV
-80.2367 eV = -68.3929 eV (uncorrected energy) - 7.6300 eV (MP Advanced Correction) - 4.2137 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)