Final Magnetic Moment9.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.295 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.113 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.88 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToV3O5 + Li3VO4 + Fe2O3 + V2O3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 -1> | 286.9 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 208.1 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 237.0 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 130.1 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 298.4 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 245.1 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 234.1 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 156.1 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 290.4 |
CeO2 (mp-20194) | <1 0 0> | <1 0 -1> | 143.5 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 286.1 |
GaAs (mp-2534) | <1 0 0> | <1 0 -1> | 95.6 |
GaAs (mp-2534) | <1 1 1> | <1 0 -1> | 286.9 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 208.1 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 234.1 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 364.2 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 234.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 -1> | 239.1 |
GaSe (mp-1943) | <1 0 0> | <1 1 -1> | 265.8 |
GaSe (mp-1943) | <1 1 0> | <1 0 0> | 234.1 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 182.1 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 130.1 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 78.0 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 260.1 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 234.1 |
BN (mp-984) | <1 0 0> | <1 0 -1> | 95.6 |
BN (mp-984) | <1 1 0> | <1 1 -1> | 265.8 |
BN (mp-984) | <1 1 1> | <1 0 0> | 338.2 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 234.1 |
LiNbO3 (mp-3731) | <1 0 1> | <1 0 1> | 245.1 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 338.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 245.1 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 338.9 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 286.1 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 208.1 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 234.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 0> | 316.0 |
Al (mp-134) | <1 1 0> | <1 0 0> | 156.1 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 312.1 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 223.8 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 -1> | 191.3 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 130.1 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 104.0 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 312.1 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 130.1 |
TeO2 (mp-2125) | <1 1 1> | <1 0 0> | 104.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 145.2 |
ZnSe (mp-1190) | <1 0 0> | <1 0 -1> | 95.6 |
ZnSe (mp-1190) | <1 1 1> | <1 0 -1> | 286.9 |
SiC (mp-7631) | <1 1 1> | <1 0 1> | 245.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca2ZnN2 (mp-8818) | 0.7290 | 0.000 | 3 |
Na2HgO2 (mp-4961) | 0.6439 | 0.000 | 3 |
Li(CuO)2 (mp-18162) | 0.7406 | 0.005 | 3 |
Li(CuO)2 (mp-553966) | 0.6943 | 0.015 | 3 |
Li2TiV3O8 (mp-776619) | 0.2769 | 0.066 | 4 |
Li2V3NiO8 (mp-776203) | 0.1362 | 0.073 | 4 |
Li2V3CoO8 (mp-777304) | 0.1738 | 0.269 | 4 |
Li2NbV3O8 (mp-776672) | 0.4034 | 0.092 | 4 |
Li2V3CrO8 (mp-849964) | 0.2157 | 0.070 | 4 |
Mn3N2 (mp-12857) | 0.7254 | 0.096 | 2 |
Mn3N2 (mp-990207) | 0.7351 | 0.096 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eVFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv V_pv Fe_pv O |
Final Energy/Atom-6.9897 eV |
Corrected Energy-111.2530 eV
-111.2530 eV = -97.8557 eV (uncorrected energy) - 7.7790 eV (MP Advanced Correction) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)