Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.421 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.093 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.57 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToV3O5 + Li3VO4 + V2O3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [148] |
Hall-R 3 |
Point Group1 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 206.7 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 324.8 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 236.2 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 206.7 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 170.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 170.7 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 170.7 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 236.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 147.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 118.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 29.5 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 206.7 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 354.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 147.6 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 118.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 29.5 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 265.7 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 206.7 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 170.7 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 236.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 118.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 88.6 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 324.8 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 206.7 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 265.7 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 324.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 256.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 236.2 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 206.7 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 206.7 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 265.7 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 88.6 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 118.1 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 29.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 118.1 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 88.6 |
BN (mp-984) | <1 0 1> | <0 0 1> | 324.8 |
BN (mp-984) | <1 1 1> | <1 0 1> | 270.9 |
BN (mp-984) | <0 0 1> | <0 0 1> | 88.6 |
BN (mp-984) | <1 1 0> | <0 0 1> | 265.7 |
Al (mp-134) | <1 1 0> | <0 0 1> | 118.1 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 206.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 206.7 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 324.8 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 265.7 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 256.0 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 236.2 |
Al (mp-134) | <1 0 0> | <0 0 1> | 147.6 |
Al (mp-134) | <1 1 1> | <0 0 1> | 29.5 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 354.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li4Ti3O8 (mp-758836) | 0.3210 | 0.099 | 3 |
Li6Zr2O7 (mp-5418) | 0.3235 | 0.000 | 3 |
Li4Mo3O8 (mp-690551) | 0.3539 | 0.046 | 3 |
Li6Hf2O7 (mp-772185) | 0.3042 | 0.000 | 3 |
Li4Fe3O8 (mp-771986) | 0.2257 | 0.089 | 3 |
Li4Mn2Ni3O10 (mp-762854) | 0.3330 | 0.075 | 4 |
Li4Co2Ni3O10 (mp-779900) | 0.3524 | 0.245 | 4 |
Li3MgNi3O8 (mp-772324) | 0.3245 | 0.065 | 4 |
Li3Fe3SiO8 (mp-761991) | 0.2673 | 0.093 | 4 |
Li3Cr3SiO8 (mp-773368) | 0.2629 | 0.051 | 4 |
Ti9S10 (mp-673637) | 0.4916 | 0.039 | 2 |
Fe10O11 (mp-764330) | 0.4695 | 0.057 | 2 |
Fe8O9 (mp-763787) | 0.4802 | 0.063 | 2 |
Fe9O10 (mp-763441) | 0.5048 | 0.350 | 2 |
Ti9O8 (mp-32544) | 0.4395 | 0.162 | 2 |
Li6Mn3Cr2Fe3O16 (mp-861553) | 0.4800 | 0.882 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv O |
Final Energy/Atom-6.6746 eV |
Corrected Energy-221.5671 eV
-221.5671 eV = -200.2385 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 10.0920 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)