material

TiMn3O8

ID:

mp-771789

DOI:

10.17188/1300842


Material Details

Final Magnetic Moment
9.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Ferri
Formation Energy / Atom
-2.143 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.095 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.00 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
TiO2 + MnO2
Band Gap
1.436 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3m [166]
Hall
-R 3 2"
Point Group
3m
Crystal System
trigonal

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.001 204.9
AlN (mp-661) <0 0 1> <0 0 1> 0.003 263.4
C (mp-48) <0 0 1> <0 0 1> 0.005 204.9
BN (mp-984) <0 0 1> <0 0 1> 0.006 87.8
ZnO (mp-2133) <0 0 1> <0 0 1> 0.007 263.4
GaN (mp-804) <0 0 1> <0 0 1> 0.012 117.1
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.015 87.8
GaSe (mp-1943) <0 0 1> <0 0 1> 0.016 87.8
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.020 87.8
C (mp-66) <1 0 0> <0 0 1> 0.027 204.9
BaTiO3 (mp-5986) <1 0 1> <0 0 1> 0.027 117.1
C (mp-66) <1 1 1> <0 0 1> 0.027 87.8
GdScO3 (mp-5690) <1 0 0> <0 0 1> 0.030 234.2
WSe2 (mp-1821) <1 1 1> <0 0 1> 0.047 87.8
TbScO3 (mp-31119) <1 0 1> <1 0 0> 0.048 168.5
CeO2 (mp-20194) <1 1 1> <0 0 1> 0.048 204.9
Si (mp-149) <1 1 1> <0 0 1> 0.053 204.9
SiC (mp-11714) <0 0 1> <0 0 1> 0.055 204.9
GdScO3 (mp-5690) <1 0 1> <1 0 0> 0.057 168.5
SiC (mp-7631) <0 0 1> <0 0 1> 0.061 204.9
MgAl2O4 (mp-3536) <1 1 1> <0 0 1> 0.063 117.1
TbScO3 (mp-31119) <0 0 1> <1 0 0> 0.070 252.7
Ga2O3 (mp-886) <1 0 0> <0 0 1> 0.073 234.2
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.073 263.4
LiF (mp-1138) <1 1 1> <0 0 1> 0.073 29.3
DyScO3 (mp-31120) <1 0 1> <1 0 0> 0.079 168.5
DyScO3 (mp-31120) <0 0 1> <1 0 0> 0.080 252.7
TeO2 (mp-2125) <1 0 1> <0 0 1> 0.080 234.2
Ge (mp-32) <1 0 0> <1 0 0> 0.091 168.5
Ag (mp-124) <1 1 0> <1 1 0> 0.098 145.9
GaAs (mp-2534) <1 1 0> <0 0 1> 0.098 234.2
TbScO3 (mp-31119) <1 0 0> <0 0 1> 0.101 234.2
Ge (mp-32) <1 1 0> <0 0 1> 0.103 234.2
ZnSe (mp-1190) <1 1 0> <0 0 1> 0.104 234.2
LiF (mp-1138) <1 0 0> <0 0 1> 0.108 322.0
PbSe (mp-2201) <1 1 1> <0 0 1> 0.115 204.9
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.120 204.9
LiF (mp-1138) <1 1 0> <0 0 1> 0.121 117.1
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.126 29.3
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.127 29.3
C (mp-66) <1 1 0> <1 1 0> 0.130 145.9
Au (mp-81) <1 1 0> <1 1 0> 0.136 145.9
LiGaO2 (mp-5854) <0 1 0> <0 0 1> 0.142 263.4
MgO (mp-1265) <1 0 0> <0 0 1> 0.146 322.0
CdS (mp-672) <1 1 0> <0 0 1> 0.149 351.2
GaSb (mp-1156) <1 1 1> <0 0 1> 0.152 204.9
GaAs (mp-2534) <1 0 0> <1 0 0> 0.152 168.5
Cu (mp-30) <1 1 0> <0 0 1> 0.152 146.4
DyScO3 (mp-31120) <1 0 0> <0 0 1> 0.161 234.2
AlN (mp-661) <1 1 0> <0 0 1> 0.174 322.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
177 49 42 14 0 0
49 177 42 -14 -0 0
42 42 213 0 -0 0
14 -14 0 55 0 -0
0 -0 -0 0 55 14
0 0 0 -0 14 64
Compliance Tensor Sij (10-12Pa-1)
6.5 -1.7 -1 -2.2 0 0
-1.7 6.5 -1 2.2 0 0
-1 -1 5.1 0 0 0
-2.2 2.2 0 19.3 0 0
0 0 0 0 19.3 -4.3
0 0 0 0 -4.3 16.6
Shear Modulus GV
64 GPa
Bulk Modulus KV
93 GPa
Shear Modulus GR
59 GPa
Bulk Modulus KR
92 GPa
Shear Modulus GVRH
61 GPa
Bulk Modulus KVRH
92 GPa
Elastic Anisotropy
0.37
Poisson's Ratio
0.23

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
13
U Values
Mn: 3.9 eV
Pseudopotentials
VASP PAW: Ti_pv Mn_pv O
Final Energy/Atom
-7.4928 eV
Corrected Energy
-100.5739 eV
-100.5739 eV = -89.9131 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction) - 5.0426 eV (MP Advanced Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
User remarks:
  • supplementary compounds from MIT matgen database

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)