Final Magnetic Moment2.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.802 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.283 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.80 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2SnO3 + Fe2O3 |
Band Gap1.997 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmce [64] |
Hall-C 2bc 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 139.5 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 232.6 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 263.2 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 279.1 |
TeO2 (mp-2125) | <0 1 0> | <1 0 0> | 271.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 325.6 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 157.9 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 271.7 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 46.5 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 140.5 |
CeO2 (mp-20194) | <1 1 1> | <0 1 1> | 210.7 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 93.0 |
TiO2 (mp-2657) | <0 0 1> | <0 1 0> | 105.3 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 263.2 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 232.6 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 279.1 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 139.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 279.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 186.1 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 325.6 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 232.6 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 232.6 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 232.6 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 263.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 271.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 325.6 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 325.6 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 325.6 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 232.6 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 139.5 |
C (mp-66) | <1 0 0> | <0 0 1> | 232.6 |
C (mp-66) | <1 1 0> | <0 0 1> | 93.0 |
C (mp-66) | <1 1 1> | <0 1 0> | 263.2 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 271.7 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 263.2 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 0> | 271.7 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 186.1 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 325.6 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 139.5 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 232.6 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 271.7 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 139.5 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 325.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 281.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 209.5 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 263.2 |
LiF (mp-1138) | <1 0 0> | <0 1 1> | 281.0 |
LaF3 (mp-905) | <1 0 1> | <1 0 0> | 271.7 |
GaP (mp-2490) | <1 1 1> | <0 1 1> | 210.7 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 209.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2Cr3O6 (mp-771534) | 0.2095 | 0.098 | 3 |
Li5Fe5O12 (mp-771687) | 0.2624 | 0.092 | 3 |
Li2Mn3O6 (mp-773276) | 0.2594 | 0.098 | 3 |
Li2(NiO2)3 (mp-773252) | 0.2927 | 0.241 | 3 |
TlIn5S7 (mp-562480) | 0.5663 | 0.000 | 3 |
Li2Mn2CoO6 (mp-775088) | 0.1874 | 0.076 | 4 |
Li2Mn2CrO6 (mp-775059) | 0.1677 | 0.100 | 4 |
Li2Fe2NiO6 (mp-777153) | 0.1760 | 0.340 | 4 |
Li2Cr2SnO6 (mp-771865) | 0.1468 | 0.078 | 4 |
Li2Mn2FeO6 (mp-774086) | 0.1659 | 0.107 | 4 |
In6Se7 (mp-567596) | 0.6386 | 0.042 | 2 |
In6S7 (mp-555853) | 0.5747 | 0.008 | 2 |
Li4Ti2Mn3(Fe2O9)2 (mp-769444) | 0.6689 | 0.081 | 5 |
Li4Ti4MnCr4O18 (mp-769442) | 0.6376 | 0.092 | 5 |
Li4Ti4Mn(Fe2O9)2 (mp-769443) | 0.6715 | 0.087 | 5 |
Li4Ti4VCr4O18 (mp-775391) | 0.6661 | 0.085 | 5 |
Li4Ti2Fe4(CoO6)3 (mp-776197) | 0.6335 | 0.217 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv Sn_d O |
Final Energy/Atom-5.8721 eV |
Corrected Energy-148.5449 eV
-148.5449 eV = -129.1854 eV (uncorrected energy) - 10.9320 eV (MP Advanced Correction) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)