Final Magnetic Moment18.973 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.079 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.057 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.77 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2MnO3 + Mn3O4 + SnO2 |
Band Gap0.009 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 302.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 323.0 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 193.8 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 267.0 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 181.5 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 267.0 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 323.0 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 258.4 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 207.9 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 193.8 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 267.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 241.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 207.9 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 258.4 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 323.0 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 323.0 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 207.9 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 302.4 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 323.0 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 323.0 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 193.8 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 193.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 258.4 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 302.4 |
BN (mp-984) | <1 0 0> | <1 0 0> | 302.4 |
BN (mp-984) | <1 1 1> | <1 0 0> | 302.4 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 193.8 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 1> | 267.0 |
MoS2 (mp-1434) | <1 0 0> | <0 1 0> | 207.9 |
Al (mp-134) | <1 0 0> | <1 0 0> | 241.9 |
Al (mp-134) | <1 1 0> | <0 1 0> | 207.9 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 323.0 |
SiC (mp-7631) | <0 0 1> | <1 0 1> | 267.0 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 181.5 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 193.8 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 193.8 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 129.2 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 181.5 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 129.2 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 64.6 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 302.4 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 258.4 |
C (mp-66) | <1 0 0> | <1 0 0> | 302.4 |
C (mp-66) | <1 1 0> | <1 0 0> | 181.5 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 181.5 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 129.2 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 323.0 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 181.5 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 258.4 |
InP (mp-20351) | <1 0 0> | <1 0 1> | 178.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li(FeO2)2 (mp-771571) | 0.1846 | 0.666 | 3 |
Ca(AgO2)2 (mvc-5243) | 0.2004 | 0.235 | 3 |
Ca(WO2)2 (mvc-6346) | 0.1886 | 0.665 | 3 |
Ca(MoO2)2 (mvc-6227) | 0.1844 | 0.228 | 3 |
Zn7(SbO6)2 (mp-675797) | 0.2160 | 0.009 | 3 |
Li4Ni5Sb3O16 (mp-762510) | 0.1610 | 0.055 | 4 |
Li4Mn3Fe5O16 (mp-772388) | 0.1614 | 0.048 | 4 |
Li4Fe5Co3O16 (mp-773387) | 0.1578 | 0.072 | 4 |
Li4Fe3Ni5O16 (mp-773324) | 0.1592 | 0.224 | 4 |
Li4Co3Sn5O16 (mp-772511) | 0.1084 | 0.026 | 4 |
Fe3O4 (mp-715491) | 0.3480 | 0.017 | 2 |
Fe3O4 (mp-542433) | 0.3417 | 0.075 | 2 |
Cr3N4 (mp-1014358) | 0.3404 | 0.227 | 2 |
Fe3O4 (mp-650112) | 0.3110 | 0.060 | 2 |
Fe3O4 (mp-716052) | 0.3474 | 0.781 | 2 |
Li4Cr3Ni2Sn3O16 (mp-775694) | 0.1327 | 0.081 | 5 |
Li4Mn3Co2Sn3O16 (mp-775606) | 0.0996 | 0.073 | 5 |
Li4Mn3Ni2Sn3O16 (mp-775346) | 0.1100 | 0.070 | 5 |
Li4Mn2Nb3Fe3O16 (mp-769626) | 0.1269 | 0.107 | 5 |
Li4Ti3Fe2Sn3O16 (mp-778363) | 0.1226 | 0.067 | 5 |
Li3MnFeCo(PO4)3 (mp-764931) | 0.6940 | 0.017 | 6 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.6794 | 0.014 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.6876 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.6927 | 0.057 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.6929 | 0.466 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Sn_d O |
Final Energy/Atom-6.5428 eV |
Corrected Energy-202.8386 eV
-202.8386 eV = -183.1977 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 8.4043 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)