Final Magnetic Moment0.595 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.375 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.036 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.71 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiNiO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 -1 -1> | 207.8 |
AlN (mp-661) | <1 0 0> | <1 -1 -1> | 155.9 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 233.7 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 255.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 276.6 |
CeO2 (mp-20194) | <1 1 0> | <1 -1 1> | 251.5 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 332.6 |
GaAs (mp-2534) | <1 0 0> | <1 1 -1> | 159.2 |
AlN (mp-661) | <0 0 1> | <0 1 -1> | 183.0 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 186.6 |
GaN (mp-804) | <1 0 0> | <1 -1 0> | 133.6 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 75.4 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 154.6 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 175.3 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 292.2 |
KCl (mp-23193) | <1 1 0> | <1 -1 0> | 178.1 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 292.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 182.5 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 -1> | 212.2 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 -1> | 318.4 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 226.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 176.0 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 147.8 |
ZnSe (mp-1190) | <1 0 0> | <1 1 -1> | 159.2 |
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 154.6 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 255.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 -1> | 159.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 1> | 257.7 |
KCl (mp-23193) | <1 0 0> | <1 -1 -1> | 207.8 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 184.8 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 149.2 |
DyScO3 (mp-31120) | <1 1 0> | <1 -1 1> | 251.5 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 226.3 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 292.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 -1 1> | 201.2 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 150.9 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 100.6 |
CdS (mp-672) | <1 0 0> | <0 1 -1> | 256.2 |
CdS (mp-672) | <1 0 1> | <1 -1 -1> | 259.8 |
LiF (mp-1138) | <1 0 0> | <1 -1 -1> | 259.8 |
LiF (mp-1138) | <1 1 1> | <0 1 1> | 257.7 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 100.6 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 255.6 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 332.6 |
YVO4 (mp-19133) | <1 0 1> | <1 0 1> | 201.5 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 201.2 |
TePb (mp-19717) | <1 0 0> | <1 -1 -1> | 207.8 |
TePb (mp-19717) | <1 1 0> | <1 -1 0> | 178.1 |
Te2Mo (mp-602) | <0 0 1> | <1 0 -1> | 298.5 |
Te2Mo (mp-602) | <1 1 0> | <0 1 0> | 295.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li4Ni5O9 (mp-767950) | 0.1727 | 0.051 | 3 |
Li13Ni15O28 (mp-761369) | 0.1799 | 0.006 | 3 |
Li13Ni15O28 (mp-769435) | 0.1855 | 0.005 | 3 |
CaFeO2 (mvc-1260) | 0.1791 | 0.612 | 3 |
Na2PrO3 (mp-28429) | 0.1898 | 0.120 | 3 |
Li5Fe2Ni3O10 (mp-771442) | 0.1585 | 0.017 | 4 |
Li5V2Fe3O10 (mp-773233) | 0.1553 | 0.049 | 4 |
Li5Ti2Fe3O10 (mp-765709) | 0.1636 | 0.026 | 4 |
Li5Ni5O9F (mp-764733) | 0.1338 | 0.070 | 4 |
Li5V2Ni3O10 (mp-781051) | 0.1648 | 0.074 | 4 |
Te2Au (mp-1662) | 0.3140 | 0.018 | 2 |
LiTe3 (mp-27466) | 0.4006 | 0.009 | 2 |
Ga2Te3 (mp-1070116) | 0.3999 | 0.334 | 2 |
Bi4Te3 (mp-28229) | 0.4160 | 0.000 | 2 |
Te2Au (mp-567525) | 0.2927 | 0.018 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.3853 | 0.139 | 5 |
Sb (mp-632286) | 0.4317 | 0.059 | 1 |
Bi (mp-567379) | 0.5798 | 0.059 | 1 |
Bi (mp-23152) | 0.5614 | 0.000 | 1 |
Te (mp-570459) | 0.3744 | 0.044 | 1 |
Te (mp-105) | 0.5507 | 0.047 | 1 |
Explore more synthesis descriptions for materials of composition LiNiO2.
Text computed by synthesisproject.org.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Ni_pv O |
Final Energy/Atom-4.8789 eV |
Corrected Energy-115.4204 eV
-115.4204 eV = -97.5775 eV (uncorrected energy) - 10.8200 eV (MP Advanced Correction) - 7.0229 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)