Final Magnetic Moment0.018 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.808 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.088 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.64 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLaCl3 + BaCl2 |
Band Gap3.403 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 213.4 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 106.7 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 155.5 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 213.4 |
Te2W (mp-22693) | <1 1 0> | <0 1 0> | 113.1 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 106.7 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 226.3 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 213.4 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 213.4 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 113.1 |
Al (mp-134) | <1 0 0> | <0 0 1> | 213.4 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 213.4 |
MgO (mp-1265) | <1 1 0> | <0 1 1> | 155.5 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 1 1> | 155.5 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 106.7 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 1 1> | 155.5 |
KP(HO2)2 (mp-23959) | <0 1 1> | <0 1 0> | 113.1 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 213.4 |
Ga2O3 (mp-886) | <1 0 1> | <0 1 0> | 226.3 |
WS2 (mp-224) | <1 0 0> | <0 1 0> | 226.3 |
ZrO2 (mp-2858) | <1 1 -1> | <0 1 0> | 226.3 |
YAlO3 (mp-3792) | <0 1 0> | <0 1 1> | 155.5 |
MgF2 (mp-1249) | <1 1 0> | <0 1 0> | 226.3 |
ZnO (mp-2133) | <1 0 0> | <0 1 0> | 226.3 |
LiAlO2 (mp-3427) | <1 1 0> | <0 1 0> | 226.3 |
LiAlO2 (mp-3427) | <1 1 1> | <0 0 1> | 106.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BaLaBr5 (mp-772891) | 0.1490 | 0.085 | 3 |
Mg2Si (mp-1074665) | 0.7374 | 0.243 | 2 |
Mg7Si4 (mp-1074846) | 0.7094 | 0.256 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv La Cl |
Final Energy/Atom-4.6834 eV |
Corrected Energy-262.2690 eV
-262.2690 eV = -262.2690 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)