Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.707 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.014 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.72 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLaI3 + BaI2 |
Band Gap2.228 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPc [7] |
HallP 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 281.2 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 140.6 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 281.2 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 281.2 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 140.6 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 210.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 281.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 140.6 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 210.9 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 140.6 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 210.9 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 140.6 |
TeO2 (mp-2125) | <1 1 1> | <0 0 1> | 210.9 |
Fe3O4 (mp-19306) | <1 1 0> | <0 0 1> | 210.9 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 281.2 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 140.6 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 210.9 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 210.9 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 281.2 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 281.2 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 281.2 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 210.9 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 210.9 |
C (mp-48) | <0 0 1> | <0 0 1> | 210.9 |
C (mp-48) | <1 0 0> | <0 0 1> | 210.9 |
C (mp-48) | <1 0 1> | <0 0 1> | 140.6 |
NaCl (mp-22862) | <1 1 0> | <0 0 1> | 140.6 |
ZrO2 (mp-2858) | <1 0 1> | <0 0 1> | 210.9 |
ZrO2 (mp-2858) | <1 1 0> | <0 0 1> | 281.2 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 210.9 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 210.9 |
ZnO (mp-2133) | <1 1 0> | <0 0 1> | 281.2 |
MgAl2O4 (mp-3536) | <1 1 0> | <0 0 1> | 281.2 |
GaSb (mp-1156) | <1 1 0> | <0 0 1> | 210.9 |
Ge (mp-32) | <1 1 0> | <0 0 1> | 140.6 |
LiAlO2 (mp-3427) | <1 0 1> | <0 0 1> | 210.9 |
Al2O3 (mp-1143) | <1 1 0> | <0 0 1> | 210.9 |
Al2O3 (mp-1143) | <1 1 1> | <0 0 1> | 210.9 |
ZnTe (mp-2176) | <1 1 0> | <0 0 1> | 210.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ba3LaCl9 (mp-771948) | 0.1522 | 0.019 | 3 |
Sr3LaCl9 (mp-771883) | 0.2512 | 0.010 | 3 |
Ba3LaBr9 (mp-772024) | 0.0746 | 0.006 | 3 |
Ba3YI9 (mp-772018) | 0.1875 | 0.048 | 3 |
Sr3YI9 (mp-771936) | 0.2471 | 0.064 | 3 |
Tm7Cl15 (mp-680292) | 0.4904 | 0.267 | 2 |
Yb7Cl15 (mp-680254) | 0.5318 | 0.004 | 2 |
Sm5Br11 (mp-680266) | 0.4642 | 0.209 | 2 |
Nd4Br9 (mp-570534) | 0.4294 | 0.151 | 2 |
Yb6Cl13 (mp-722729) | 0.5528 | 0.029 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv La I |
Final Energy/Atom-3.5848 eV |
Corrected Energy-186.4090 eV
-186.4090 eV = -186.4090 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)