Final Magnetic Moment13.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.062 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.071 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.84 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi6MnO4 + MnO + LiMnO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 0> | 170.3 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 203.8 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 305.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 271.7 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 237.8 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 169.8 |
AlN (mp-661) | <0 0 1> | <1 1 -1> | 239.2 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 195.1 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 259.0 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 203.8 |
GaN (mp-804) | <1 1 0> | <1 1 -1> | 239.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 305.7 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 195.1 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 34.0 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 305.7 |
BaF2 (mp-1029) | <1 1 1> | <1 0 1> | 262.1 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 -1> | 159.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 135.9 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 -1> | 56.0 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 224.0 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 340.6 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 169.8 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 169.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 169.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 -1> | 56.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 65.0 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 305.7 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 305.7 |
InAs (mp-20305) | <1 1 1> | <1 0 1> | 262.1 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 203.8 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 271.7 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 168.0 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 169.8 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 34.0 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 237.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 65.0 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 259.0 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 262.1 |
YVO4 (mp-19133) | <1 0 0> | <1 1 -1> | 318.9 |
YVO4 (mp-19133) | <1 0 1> | <1 0 -1> | 280.0 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 169.8 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 34.0 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 271.7 |
Te2Mo (mp-602) | <0 0 1> | <1 0 -1> | 336.0 |
Te2Mo (mp-602) | <1 0 0> | <1 0 1> | 262.1 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 34.0 |
Ag (mp-124) | <1 1 0> | <1 0 -1> | 168.0 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 237.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 260.2 |
GaSe (mp-1943) | <1 0 0> | <1 0 1> | 262.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Yb(BiTe2)2 (mp-677162) | 0.5987 | 0.094 | 3 |
Yb(SbTe2)2 (mp-675892) | 0.6754 | 0.112 | 3 |
Li5(NiO2)4 (mp-780142) | 0.5827 | 0.061 | 3 |
LaYbS3 (mp-21106) | 0.6466 | 0.219 | 3 |
LaYbS3 (mp-562284) | 0.6288 | 0.219 | 3 |
Li5MnCr3O8 (mp-764183) | 0.4740 | 0.079 | 4 |
Li5V2Cr2O8 (mp-764149) | 0.6368 | 0.080 | 4 |
Li5MnV3O8 (mp-764142) | 0.5979 | 0.047 | 4 |
Li5Cr3NiO8 (mp-764140) | 0.5761 | 0.037 | 4 |
Li5Cr3FeO8 (mp-763916) | 0.6417 | 0.584 | 4 |
CaDyMnSnO6 (mp-706325) | 0.7248 | 0.211 | 5 |
NaTbMnWO6 (mp-566068) | 0.7077 | 0.109 | 5 |
NaNdMnWO6 (mp-25017) | 0.6986 | 0.109 | 5 |
NaLaMnWO6 (mp-25027) | 0.7252 | 0.114 | 5 |
CaLaFeAgO6 (mvc-8977) | 0.7271 | 0.054 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv O |
Final Energy/Atom-6.3812 eV |
Corrected Energy-241.6441 eV
-241.6441 eV = -216.9606 eV (uncorrected energy) - 13.4468 eV (MP Advanced Correction) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)