Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.299 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.026 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.30 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi4Ti5O12 + TiO2 |
Band Gap3.126 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI41/a [88] |
HallI 4bw 1bw |
Point Group4/m |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 114.5 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 114.5 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 114.5 |
TeO2 (mp-2125) | <0 1 1> | <1 0 0> | 229.0 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 229.0 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 229.0 |
TiO2 (mp-390) | <0 0 1> | <0 0 1> | 187.4 |
LiAlO2 (mp-3427) | <1 0 0> | <1 0 0> | 229.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiMnF3 (mp-779183) | 0.5716 | 0.527 | 3 |
Li2FeF4 (mp-853234) | 0.5416 | 0.157 | 3 |
Li2FeF4 (mp-778700) | 0.5336 | 0.271 | 3 |
Ta2Zn3O8 (mp-28251) | 0.5563 | 0.000 | 3 |
LiMn2F5 (mp-774365) | 0.5624 | 0.038 | 3 |
LiCoOF2 (mp-780318) | 0.5036 | 0.223 | 4 |
Li9Fe3(WO4)7 (mp-773457) | 0.5096 | 0.051 | 4 |
Li9Mn3(WO4)7 (mp-777686) | 0.5238 | 0.170 | 4 |
Li9V3(WO4)7 (mp-777624) | 0.5320 | 0.088 | 4 |
LiVOF2 (mp-765336) | 0.5521 | 0.054 | 4 |
Mn2O3 (mp-771717) | 0.7036 | 0.088 | 2 |
Fe2O3 (mp-628327) | 0.6676 | 0.749 | 2 |
Al2O3 (mp-2254) | 0.6884 | 0.017 | 2 |
Ga2O3 (mp-886) | 0.7169 | 0.000 | 2 |
Fe2O3 (mp-715516) | 0.6791 | 0.749 | 2 |
Li9TiMn3(PO4)6 (mp-770123) | 0.7404 | 0.078 | 5 |
Li4TiCu3(PO4)4 (mp-760136) | 0.7001 | 0.090 | 5 |
Li3Mn2P2(O4F)2 (mp-763234) | 0.7102 | 0.024 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Ti_pv O |
Final Energy/Atom-8.2571 eV |
Corrected Energy-573.0587 eV
-573.0587 eV = -544.9671 eV (uncorrected energy) - 28.0916 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)