Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.751 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.029 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.52 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCu3(CO4)2 + Na2S2O7 + CO2 + O2 |
Band Gap0.442 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 0 1> | 108.6 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 222.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 325.9 |
AlN (mp-661) | <0 0 1> | <1 0 1> | 297.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 108.6 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 286.6 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 311.0 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 144.9 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 289.7 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 108.6 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 297.1 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 318.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 289.7 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 311.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 108.6 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 222.2 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 190.8 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 311.0 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 253.5 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 108.6 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 318.0 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 222.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 253.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 144.9 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 253.5 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 286.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 217.3 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 72.4 |
Te2W (mp-22693) | <0 0 1> | <0 1 1> | 172.0 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 108.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 355.5 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 1> | 173.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 310.3 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 253.5 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 325.9 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 217.3 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 222.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 108.6 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 259.7 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 297.1 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 144.9 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 72.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 144.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 311.0 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 253.5 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 289.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 72.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 181.1 |
BN (mp-984) | <1 0 0> | <0 0 1> | 289.7 |
BN (mp-984) | <1 1 1> | <0 1 1> | 229.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na3Ca(BO2)5 (mp-542719) | 0.7405 | 0.000 | 4 |
CaGaBO4 (mp-557855) | 0.7494 | 0.000 | 4 |
YbCu2(MoO4)3 (mp-565220) | 0.7481 | 0.046 | 4 |
LiSn10(PO4)7 (mp-765193) | 0.6766 | 0.086 | 4 |
MnZnPO5 (mvc-3247) | 0.7260 | 0.029 | 4 |
Na2MnBSO7 (mp-771504) | 0.4540 | 0.155 | 5 |
Na2MnPCO7 (mp-780530) | 0.4849 | 0.134 | 5 |
Na2NiPCO7 (mp-775619) | 0.4935 | 0.040 | 5 |
Na2MnPCO7 (mp-775499) | 0.5231 | 0.136 | 5 |
Na2CuBSO7 (mp-771122) | 0.3379 | 0.082 | 5 |
Na2LiMnPCO7 (mp-764273) | 0.7497 | 0.084 | 6 |
KLiMnPCO7 (mp-764256) | 0.7127 | 0.000 | 6 |
NaLiMnPCO7 (mp-763833) | 0.5709 | 0.062 | 6 |
NaLi2MnPCO7 (mp-773802) | 0.7250 | 0.084 | 6 |
KLi2MnPCO7 (mp-764310) | 0.7118 | 0.070 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Cu_pv C S O |
Final Energy/Atom-6.0994 eV |
Corrected Energy-144.8116 eV
Uncorrected energy = -134.1876 eV
Composition-based energy adjustment (-0.503 eV/atom x 2.0 atoms) = -1.0060 eV
Composition-based energy adjustment (-0.687 eV/atom x 14.0 atoms) = -9.6180 eV
Corrected energy = -144.8116 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)