Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.865 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.38 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.599 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI41/amd [141] |
HallI 4bw 2bw 1bw |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 134.8 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 63.5 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 317.7 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 224.7 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 134.8 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 314.5 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 317.7 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 201.5 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 270.0 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 251.9 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 224.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 254.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 251.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 151.1 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 254.2 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 202.5 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 224.7 |
Te2W (mp-22693) | <1 0 0> | <1 1 0> | 190.6 |
Te2W (mp-22693) | <1 1 0> | <1 0 0> | 224.7 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 44.9 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 63.5 |
Te2Mo (mp-602) | <1 1 1> | <1 1 0> | 190.6 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 224.7 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 269.6 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 151.1 |
BN (mp-984) | <1 0 0> | <0 0 1> | 151.1 |
Al (mp-134) | <1 1 0> | <1 1 0> | 254.2 |
Al (mp-134) | <1 1 1> | <0 0 1> | 251.9 |
LiGaO2 (mp-5854) | <0 1 0> | <1 1 0> | 63.5 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 0> | 190.6 |
SiC (mp-7631) | <1 0 1> | <1 1 0> | 190.6 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 202.5 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 314.5 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 224.7 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 251.9 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 251.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 201.5 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 134.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 179.7 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 224.7 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 1> | 270.0 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 251.9 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 1> | 162.2 |
InAs (mp-20305) | <1 0 0> | <1 1 0> | 190.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 251.9 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 134.8 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 224.7 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 0 1> | 151.1 |
LaF3 (mp-905) | <1 0 1> | <1 0 0> | 134.8 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 314.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YAsO4 (mp-8058) | 0.0531 | 0.000 | 3 |
DyAsO4 (mp-5632) | 0.0430 | 0.000 | 3 |
TmAsO4 (mp-771977) | 0.0394 | 0.000 | 3 |
CeVO4 (mp-19214) | 0.0278 | 0.056 | 3 |
HoAsO4 (mp-12944) | 0.0230 | 0.000 | 3 |
CaU(PO4)2 (mp-9360) | 0.5682 | 0.000 | 4 |
Ho2SiSO4 (mp-17366) | 0.6141 | 0.019 | 4 |
Er2SiSO4 (mp-555990) | 0.5902 | 0.020 | 4 |
Ca2AsClO4 (mp-560595) | 0.6138 | 0.000 | 4 |
PrTl(MoO4)2 (mp-19579) | 0.6133 | 0.006 | 4 |
TlCl2 (mp-27205) | 0.6197 | 0.000 | 2 |
TlBr2 (mp-27398) | 0.5115 | 0.000 | 2 |
InI2 (mp-29312) | 0.5154 | 0.000 | 2 |
InBr2 (mp-568108) | 0.5310 | 0.000 | 2 |
GaCl2 (mp-568848) | 0.5671 | 0.000 | 2 |
DyZr9Si9PO40 (mp-686636) | 0.3875 | 0.011 | 5 |
YZr5Si5PO24 (mp-532768) | 0.4178 | 0.014 | 5 |
KCaNd(PO4)2 (mp-676934) | 0.5704 | 0.000 | 5 |
YbZr7Si7PO32 (mp-690946) | 0.4389 | 0.019 | 5 |
ErZr11Si11PO48 (mp-690951) | 0.3584 | 0.008 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Er_3 As O |
Final Energy/Atom-7.2329 eV |
Corrected Energy-92.4136 eV
-92.4136 eV = -86.7953 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)