Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.511 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.075 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.09 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLaI3 + CaI2 |
Band Gap2.149 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 0> | <0 1 0> | 255.2 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 208.7 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 170.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 278.3 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 278.3 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 278.3 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 208.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 278.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 255.2 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 278.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 278.3 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 278.3 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 170.1 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 170.1 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 255.2 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 278.3 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 278.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 69.6 |
Bi2Te3 (mp-34202) | <1 0 0> | <0 0 1> | 139.2 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 255.2 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 255.2 |
BN (mp-984) | <1 1 1> | <0 0 1> | 69.6 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 278.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 208.7 |
BN (mp-984) | <1 1 0> | <0 0 1> | 69.6 |
Al (mp-134) | <1 1 0> | <0 1 0> | 255.2 |
CdTe (mp-406) | <1 1 0> | <0 1 0> | 255.2 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 278.3 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 208.7 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 208.7 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 278.3 |
InSb (mp-20012) | <1 1 0> | <0 1 0> | 255.2 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 278.3 |
PbSe (mp-2201) | <1 1 0> | <0 1 0> | 170.1 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 208.7 |
MoSe2 (mp-1634) | <1 0 0> | <0 0 1> | 208.7 |
Si (mp-149) | <1 1 0> | <0 0 1> | 208.7 |
Si (mp-149) | <1 1 1> | <0 0 1> | 208.7 |
Au (mp-81) | <1 1 1> | <0 0 1> | 278.3 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 278.3 |
CdSe (mp-2691) | <1 1 0> | <0 1 0> | 170.1 |
YAlO3 (mp-3792) | <0 1 1> | <0 0 1> | 139.2 |
SiC (mp-8062) | <1 1 0> | <0 1 1> | 109.9 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 278.3 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 278.3 |
MgF2 (mp-1249) | <1 1 0> | <0 0 1> | 208.7 |
GaSb (mp-1156) | <1 0 0> | <0 0 1> | 278.3 |
GaSb (mp-1156) | <1 1 0> | <0 1 0> | 170.1 |
Cu (mp-30) | <1 1 0> | <0 0 1> | 278.3 |
CaF2 (mp-2741) | <1 1 1> | <0 0 1> | 208.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LaMgI5 (mp-756448) | 0.5087 | 0.017 | 3 |
CaLaI5 (mp-770473) | 0.5902 | 0.024 | 3 |
CaLaI5 (mp-755779) | 0.3202 | 0.071 | 3 |
CaLaI5 (mp-772082) | 0.6249 | 0.025 | 3 |
Ca3Pb3I14 (mp-771877) | 0.6373 | 0.096 | 3 |
SrLiFeF6 (mp-567062) | 0.6784 | 0.000 | 4 |
SrLiCoF6 (mp-567434) | 0.6689 | 0.000 | 4 |
SrLiCoF6 (mp-567464) | 0.7252 | 0.000 | 4 |
Ti7Cl16 (mp-540671) | 0.7171 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv La I |
Final Energy/Atom-3.5921 eV |
Corrected Energy-100.5790 eV
-100.5790 eV = -100.5790 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)