Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.436 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.003 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.22 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSb3IO4 + SbI3 |
Band Gap1.932 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 338.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 187.8 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 172.6 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 300.5 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 79.6 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 112.7 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 338.1 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 222.1 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 159.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 338.1 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 86.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 338.1 |
SiO2 (mp-6930) | <1 0 0> | <1 1 -1> | 253.3 |
SiO2 (mp-6930) | <1 1 1> | <1 1 1> | 262.0 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 238.7 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 86.3 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 159.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 259.0 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 222.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 295.7 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 338.1 |
Te2W (mp-22693) | <1 1 0> | <0 0 1> | 112.7 |
Te2Mo (mp-602) | <1 0 0> | <1 0 -1> | 159.1 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 295.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 225.4 |
BN (mp-984) | <1 0 1> | <1 1 1> | 262.0 |
BN (mp-984) | <1 1 0> | <0 0 1> | 300.5 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 187.8 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 0> | 74.0 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 -1> | 253.3 |
CdTe (mp-406) | <1 1 0> | <1 0 -1> | 238.7 |
SiC (mp-7631) | <1 0 0> | <1 0 -1> | 238.7 |
SiC (mp-7631) | <1 0 1> | <1 0 -1> | 318.3 |
SiC (mp-7631) | <1 1 0> | <1 0 -1> | 79.6 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 338.1 |
TiO2 (mp-2657) | <1 1 1> | <1 1 1> | 262.0 |
C (mp-66) | <1 0 0> | <1 0 1> | 259.0 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 -1> | 238.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 -1> | 238.7 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 259.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 150.3 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 246.5 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 150.3 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 259.0 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 159.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 1> | 131.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 338.1 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 338.1 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 263.0 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 112.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sb I O |
Final Energy/Atom-5.1442 eV |
Corrected Energy-121.5574 eV
Uncorrected energy = -113.1714 eV
Composition-based energy adjustment (-0.687 eV/atom x 10.0 atoms) = -6.8700 eV
Composition-based energy adjustment (-0.379 eV/atom x 4.0 atoms) = -1.5160 eV
Corrected energy = -121.5574 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)