Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.466 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.092 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.89 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiFePO4 |
Band Gap3.364 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinImma [74] |
Hall-I 2b 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 331.6 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 198.4 |
AlN (mp-661) | <1 1 0> | <1 1 1> | 222.3 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 200.6 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 264.5 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 46.1 |
GaAs (mp-2534) | <1 1 1> | <0 1 0> | 230.7 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 230.7 |
AlN (mp-661) | <1 0 0> | <1 1 1> | 222.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 33.4 |
BaF2 (mp-1029) | <1 0 0> | <1 1 0> | 330.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 234.1 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 189.5 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 133.8 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 92.3 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 148.2 |
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 171.0 |
SiO2 (mp-6930) | <1 0 0> | <1 1 1> | 222.3 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 138.4 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 330.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 92.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 132.3 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 1> | 222.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 46.1 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 58.0 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 66.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 300.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 33.4 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 46.1 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 230.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 33.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 46.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 1> | 57.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 334.4 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 200.6 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 230.7 |
CdS (mp-672) | <1 1 0> | <0 1 1> | 341.9 |
CdS (mp-672) | <1 1 1> | <1 1 0> | 264.5 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 33.4 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 46.1 |
LiF (mp-1138) | <1 1 1> | <0 1 1> | 57.0 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 300.9 |
YVO4 (mp-19133) | <0 0 1> | <1 1 0> | 264.5 |
YVO4 (mp-19133) | <1 0 1> | <1 0 1> | 289.9 |
TePb (mp-19717) | <1 0 0> | <1 1 0> | 330.7 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 184.6 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 300.9 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 138.4 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 47.4 |
Ag (mp-124) | <1 1 1> | <1 0 1> | 58.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Al(SnO2)2 (mvc-4103) | 0.1713 | 0.427 | 3 |
Cd2SiO4 (mp-560842) | 0.1447 | 0.134 | 3 |
Na2WO4 (mp-18803) | 0.1447 | 0.000 | 3 |
Na2MoO4 (mp-18852) | 0.1150 | 0.000 | 3 |
Ag2MoO4 (mp-19318) | 0.1243 | 0.001 | 3 |
LiNiPO4 (mp-767362) | 0.1911 | 0.079 | 4 |
LiVPO4 (mp-774020) | 0.1234 | 0.071 | 4 |
LiFePO4 (mp-766765) | 0.1971 | 0.088 | 4 |
LiNiPO4 (mp-762914) | 0.2066 | 0.078 | 4 |
LiMnPO4 (mp-18997) | 0.3924 | 0.000 | 4 |
Fe3S4 (mp-850016) | 0.7284 | 0.144 | 2 |
Cr3N4 (mp-1014379) | 0.7299 | 0.105 | 2 |
Mn3N4 (mp-1080204) | 0.6966 | 0.172 | 2 |
Cr3N4 (mp-1014358) | 0.6842 | 0.226 | 2 |
Re3N4 (mp-1080201) | 0.7250 | 0.110 | 2 |
Li2MnFe(PO4)2 (mp-775189) | 0.4082 | 0.020 | 5 |
Li4Fe3Co(PO4)4 (mp-762290) | 0.4083 | 0.011 | 5 |
Li4MnFe3(PO4)4 (mp-767478) | 0.4024 | 0.001 | 5 |
Li2MnFe(PO4)2 (mp-764670) | 0.4086 | 0.003 | 5 |
Li4MnFe3(PO4)4 (mp-783919) | 0.4055 | 0.015 | 5 |
Li3MnFeCo(PO4)3 (mp-764804) | 0.4257 | 0.043 | 6 |
Li3MnFeCo(PO4)3 (mp-764707) | 0.4327 | 0.035 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.4324 | 0.057 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.4288 | 0.466 | 6 |
Li3MnFeCo(PO4)3 (mp-764867) | 0.4314 | 0.031 | 6 |
Explore more synthesis descriptions for materials of composition LiFePO4.
Text computed by synthesisproject.org.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv P O |
Final Energy/Atom-6.7572 eV |
Corrected Energy-211.3716 eV
-211.3716 eV = -189.2029 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 10.9320 eV (MP Advanced Correction)
|