Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.547 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.063 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.16 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBiO2 + Y2O3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 237.2 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 161.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 47.4 |
InAs (mp-20305) | <1 1 1> | <1 0 -1> | 260.5 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 260.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 332.1 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 332.1 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 100.1 |
LiF (mp-1138) | <1 1 1> | <1 1 -1> | 143.2 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 284.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 332.1 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 189.8 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 100.1 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 47.4 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 237.2 |
BaF2 (mp-1029) | <1 1 1> | <1 0 -1> | 260.5 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 332.1 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 142.3 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 94.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 284.7 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 332.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 100.1 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 47.4 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 237.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 47.4 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 237.2 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 47.4 |
Te2W (mp-22693) | <0 1 0> | <1 0 -1> | 260.5 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 189.8 |
Te2Mo (mp-602) | <1 0 0> | <1 0 -1> | 260.5 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 237.2 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 47.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 237.2 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 189.8 |
GaSe (mp-1943) | <1 0 0> | <1 0 1> | 200.2 |
BN (mp-984) | <0 0 1> | <0 0 1> | 189.8 |
BN (mp-984) | <1 0 1> | <0 0 1> | 237.2 |
BN (mp-984) | <1 1 0> | <1 0 -1> | 260.5 |
BN (mp-984) | <1 1 1> | <0 0 1> | 237.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 237.2 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 237.2 |
Al (mp-134) | <1 0 0> | <1 0 -1> | 260.5 |
Al (mp-134) | <1 1 0> | <0 0 1> | 47.4 |
Al (mp-134) | <1 1 1> | <1 1 -1> | 143.2 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 332.1 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 332.1 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 189.8 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 94.9 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 142.3 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 237.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sc2Ti2O7 (mp-780402) | 0.4568 | 0.057 | 3 |
Ho2Zr2O7 (mp-770289) | 0.4951 | 0.073 | 3 |
Dy2Zr2O7 (mp-772760) | 0.4691 | 0.038 | 3 |
In2Bi2O7 (mp-768468) | 0.5061 | 0.081 | 3 |
Y2Zr2O7 (mp-771043) | 0.4705 | 0.064 | 3 |
Li4Mn3OF11 (mp-766928) | 0.6759 | 0.073 | 4 |
Li3Fe4(OF3)3 (mp-777493) | 0.5868 | 0.076 | 4 |
Li3Fe4(OF3)3 (mp-776685) | 0.6620 | 0.101 | 4 |
Li2Fe5O5F7 (mp-849531) | 0.6581 | 0.097 | 4 |
Li3V4(OF3)3 (mp-766144) | 0.6645 | 0.071 | 4 |
Ti4O7 (mp-778663) | 0.7194 | 0.091 | 2 |
Na5Ca6Nd5Zr16O48 (mp-695571) | 0.7355 | 0.004 | 5 |
Cu6AgBi12PbS22 (mp-651706) | 0.6011 | 0.025 | 5 |
Mg3AlFe(SiO4)3 (mp-699146) | 0.7384 | 0.189 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Y_sv Bi O |
Final Energy/Atom-7.1323 eV |
Corrected Energy-333.4838 eV
-333.4838 eV = -313.8197 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)