material

Mn3CoO8

ID:

mp-771970


Material Details

Final Magnetic Moment
10.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-1.601 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.024 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.25 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
CoO2 + MnO2
Band Gap
1.341 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3m [166]
Hall
-R 3 2"
Point Group
3m
Crystal System
trigonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
BN (mp-984) <0 0 1> <0 0 1> 0.000 87.4
GaN (mp-804) <0 0 1> <0 0 1> 0.001 116.6
AlN (mp-661) <0 0 1> <1 0 1> 0.001 261.1
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.001 87.4
SiO2 (mp-6930) <1 0 1> <1 1 0> 0.002 142.1
GdScO3 (mp-5690) <1 0 0> <0 0 1> 0.010 233.2
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.015 204.0
BaTiO3 (mp-5986) <1 0 1> <0 0 1> 0.015 116.6
Al2O3 (mp-1143) <0 0 1> <1 0 1> 0.020 261.1
GdScO3 (mp-5690) <0 0 1> <1 0 0> 0.020 164.0
GdScO3 (mp-5690) <1 0 1> <1 0 1> 0.020 174.1
C (mp-48) <0 0 1> <0 0 1> 0.030 204.0
MgAl2O4 (mp-3536) <1 1 1> <0 0 1> 0.033 116.6
LiF (mp-1138) <1 1 1> <0 0 1> 0.041 29.1
Ge (mp-32) <1 1 0> <1 1 0> 0.047 142.1
C (mp-66) <1 0 0> <0 0 1> 0.048 204.0
WSe2 (mp-1821) <1 1 1> <1 0 1> 0.050 87.0
C (mp-66) <1 1 0> <1 1 1> 0.051 145.0
GaSe (mp-1943) <0 0 1> <0 0 1> 0.054 87.4
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.063 87.4
TbScO3 (mp-31119) <1 0 0> <0 0 1> 0.067 233.2
Ge (mp-32) <1 0 0> <1 0 0> 0.067 164.0
LiF (mp-1138) <1 0 0> <0 0 1> 0.068 320.6
TeO2 (mp-2125) <0 0 1> <1 0 0> 0.075 164.0
C (mp-66) <1 1 1> <0 0 1> 0.076 87.4
PbSe (mp-2201) <1 1 1> <0 0 1> 0.077 204.0
GaAs (mp-2534) <1 1 0> <1 1 0> 0.082 142.1
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.087 29.1
TbScO3 (mp-31119) <1 0 1> <1 0 0> 0.087 164.0
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.088 29.1
GaAs (mp-2534) <1 0 0> <1 0 0> 0.098 164.0
ZnO (mp-2133) <1 0 0> <1 0 0> 0.103 246.1
TeO2 (mp-2125) <1 0 1> <0 0 1> 0.104 233.2
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.108 142.1
GaSb (mp-1156) <1 1 1> <0 0 1> 0.110 204.0
CeO2 (mp-20194) <1 1 1> <0 0 1> 0.113 204.0
Si (mp-149) <1 1 1> <0 0 1> 0.120 204.0
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.121 164.0
SiC (mp-11714) <0 0 1> <0 0 1> 0.124 204.0
DyScO3 (mp-31120) <1 0 0> <0 0 1> 0.125 233.2
DyScO3 (mp-31120) <1 0 1> <1 0 0> 0.128 164.0
SiC (mp-7631) <0 0 1> <0 0 1> 0.133 204.0
DyScO3 (mp-31120) <0 0 1> <1 0 0> 0.135 246.1
WS2 (mp-224) <0 0 1> <0 0 1> 0.140 116.6
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.141 116.6
CdSe (mp-2691) <1 1 1> <0 0 1> 0.141 204.0
Ni (mp-23) <1 1 0> <1 0 0> 0.152 246.1
LiF (mp-1138) <1 1 0> <0 0 1> 0.187 116.6
Ga2O3 (mp-886) <1 0 0> <1 0 0> 0.197 164.0
MgO (mp-1265) <1 0 0> <0 0 1> 0.210 320.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.

Once you have registered you can also "vote" for full calculation of this material's elastic properties.

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Mn3CuO8 (mp-771796) 0.0625 0.074 3
MnCo3O8 (mp-773602) 0.0787 0.022 3
Mn3CrO8 (mp-770001) 0.0601 0.075 3
Mn7CrO16 (mp-769632) 0.0679 0.060 3
TiMn4O10 (mp-777945) 0.0848 0.082 3
Ti2Mn3Cr3O16 (mp-771540) 0.5120 0.084 4
Ti3Mn3Cr2O16 (mp-770915) 0.5264 0.098 4
Mn3Cr3(WO8)2 (mp-778921) 0.5157 0.086 4
LiV3(OF3)2 (mp-766156) 0.4791 0.082 4
Mn3Cr3(TeO8)2 (mp-772458) 0.5189 0.082 4
SnO2 (mvc-4323) 0.1189 0.191 2
CoO2 (mp-714976) 0.1020 0.008 2
TiO2 (mvc-11912) 0.0666 0.179 2
CoO2 (mp-715480) 0.0666 0.008 2
MnO2 (mp-715446) 0.0835 0.033 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
Mn: 3.9 eV
Co: 3.32 eV
Pseudopotentials
VASP PAW: Mn_pv Co O
Final Energy/Atom
-6.7705 eV
Corrected Energy
-93.3844 eV
Uncorrected energy = -81.2464 eV Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV Composition-based energy adjustment (-1.668 eV/atom x 3.0 atoms) = -5.0040 eV Composition-based energy adjustment (-1.638 eV/atom x 1.0 atoms) = -1.6380 eV Corrected energy = -93.3844 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)