Final Magnetic Moment4.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.589 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.033 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.81 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNi3O4 + Li2WO4 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63mc [186] |
HallP 6c 2c |
Point Group6mm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 239.3 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 209.4 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 269.2 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 255.4 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 338.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 89.7 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 329.0 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 209.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 239.3 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 56.4 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 239.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 239.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 358.9 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 209.4 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 282.0 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 127.7 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 269.2 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 319.2 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 209.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 169.2 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 119.6 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 29.9 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 282.0 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 195.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 119.6 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 239.3 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 119.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 225.6 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 209.4 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 169.2 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 89.7 |
GaSe (mp-1943) | <1 0 1> | <1 1 1> | 204.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 319.2 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 319.2 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 282.0 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 358.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 149.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 89.7 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 209.4 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 269.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 1> | 319.2 |
MoS2 (mp-1434) | <0 0 1> | <1 1 1> | 204.3 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 169.2 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 29.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 119.6 |
Al (mp-134) | <1 0 0> | <0 0 1> | 149.6 |
Al (mp-134) | <1 1 0> | <0 0 1> | 119.6 |
Al (mp-134) | <1 1 1> | <0 0 1> | 29.9 |
BN (mp-984) | <0 0 1> | <1 0 1> | 191.5 |
BN (mp-984) | <1 0 1> | <0 0 1> | 209.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3Fe3O8 (mp-771621) | 0.2382 | 0.145 | 3 |
Li(FeO2)2 (mp-771571) | 0.2356 | 0.666 | 3 |
LiCr2O4 (mp-771523) | 0.2468 | 0.088 | 3 |
LiTi2O4 (mp-776170) | 0.2240 | 0.042 | 3 |
Li3FeO3 (mp-770886) | 0.2403 | 0.361 | 3 |
Li2NbCr3O8 (mp-762276) | 0.1644 | 0.000 | 4 |
Li2Fe3WO8 (mp-775194) | 0.1678 | 0.324 | 4 |
Li2Ni3TeO8 (mp-772379) | 0.1413 | 0.012 | 4 |
Li2Mn3WO8 (mp-772369) | 0.1459 | 0.049 | 4 |
Li2NbV3O8 (mp-777682) | 0.1470 | 0.000 | 4 |
Fe3O4 (mp-715491) | 0.3539 | 0.017 | 2 |
Fe3O4 (mp-542433) | 0.3777 | 0.075 | 2 |
Mn3N4 (mp-1080204) | 0.3151 | 0.172 | 2 |
Cr3N4 (mp-1014358) | 0.2978 | 0.227 | 2 |
Fe3O4 (mp-650112) | 0.3517 | 0.060 | 2 |
Li4Fe3Ni3(WO8)2 (mp-772358) | 0.1712 | 0.042 | 5 |
Li4Nb2V3Cr3O16 (mp-770954) | 0.1575 | 0.007 | 5 |
Li4V3Ni3(WO8)2 (mp-777059) | 0.1599 | 0.032 | 5 |
Li4Nb2Cr3Fe3O16 (mp-772123) | 0.1751 | 1.039 | 5 |
Li4Cr3Ni3(WO8)2 (mp-761720) | 0.1747 | 0.033 | 5 |
Li3MnFeCo(PO4)3 (mp-764804) | 0.6400 | 0.043 | 6 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.6304 | 0.014 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.6365 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.6393 | 0.057 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.6361 | 0.466 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eVW: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Ni_pv W_pv O |
Final Energy/Atom-5.6772 eV |
Corrected Energy-191.8833 eV
-191.8833 eV = -158.9607 eV (uncorrected energy) - 21.6860 eV (MP Advanced Correction) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)