Final Magnetic Moment0.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.847 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.046 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.15 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNi(IO3)2 |
Band Gap2.788 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbcn [60] |
Hall-P 2n 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 1> | <0 0 1> | 143.5 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 229.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 358.7 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 229.3 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 1> | 253.3 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 322.8 |
Te2W (mp-22693) | <0 1 1> | <0 1 1> | 168.9 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 152.9 |
BN (mp-984) | <1 0 1> | <0 0 1> | 251.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 251.1 |
Al (mp-134) | <1 1 1> | <0 0 1> | 358.7 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 1> | 84.4 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 1> | 168.9 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 179.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 358.7 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 322.8 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 84.4 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 143.5 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 229.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 202.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 358.7 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 251.1 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 143.5 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 101.4 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 263.8 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 179.3 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 107.5 |
Te2W (mp-22693) | <1 1 0> | <0 1 0> | 229.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 358.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 358.7 |
BN (mp-984) | <1 0 0> | <0 1 1> | 253.3 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 322.8 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 71.7 |
MoS2 (mp-1434) | <0 0 1> | <1 1 1> | 131.9 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 286.9 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 358.7 |
LiTaO3 (mp-3666) | <0 0 1> | <0 1 0> | 229.3 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 71.7 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 305.8 |
MgO (mp-1265) | <1 1 1> | <0 1 0> | 152.9 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 286.9 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 251.1 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <0 1 0> | 152.9 |
C (mp-66) | <1 0 0> | <0 0 1> | 179.3 |
C (mp-66) | <1 1 0> | <0 1 1> | 253.3 |
C (mp-66) | <1 1 1> | <0 0 1> | 179.3 |
GdScO3 (mp-5690) | <1 1 0> | <0 1 1> | 253.3 |
Mg (mp-153) | <0 0 1> | <1 1 1> | 131.9 |
Mg (mp-153) | <1 0 0> | <0 1 1> | 84.4 |
Mg (mp-153) | <1 1 0> | <0 1 1> | 84.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CuO2F (mp-997107) | 0.3934 | 0.128 | 3 |
In(IO3)3 (mp-23400) | 0.4566 | 0.000 | 3 |
Mg(IO3)2 (mp-768315) | 0.2712 | 0.062 | 3 |
Co(IO3)2 (mp-774233) | 0.0945 | 0.145 | 3 |
Mn(IO3)2 (mp-771047) | 0.3568 | 0.041 | 3 |
LiIn(IO3)4 (mp-973966) | 0.5218 | 0.000 | 4 |
InHSeO4 (mp-560404) | 0.5587 | 0.000 | 4 |
LiV(IO4)2 (mp-566833) | 0.4990 | 0.001 | 4 |
YFe(WO4)2 (mvc-620) | 0.5430 | 0.054 | 4 |
YMn(WO4)2 (mvc-622) | 0.5104 | 0.049 | 4 |
Ni2O5 (mp-1094139) | 0.5494 | 0.533 | 2 |
MnO3 (mp-1086672) | 0.6094 | 0.512 | 2 |
TiZnH12(OF)6 (mp-866807) | 0.7438 | 0.020 | 5 |
FeH12Pt(ClO)6 (mp-542912) | 0.7029 | 0.000 | 5 |
Sr2NiSe2(ClO3)2 (mp-566796) | 0.7160 | 0.000 | 5 |
FeH12Pt(ClO)6 (mp-605175) | 0.7128 | 0.000 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Ni_pv I O |
Final Energy/Atom-4.4483 eV |
Corrected Energy-185.6501 eV
-185.6501 eV = -160.1391 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 8.6560 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)