Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.726 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.004 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.02 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiV(OF)2 |
Band Gap2.216 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 176.2 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 -1> | 238.1 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 286.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 154.2 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 139.6 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 182.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 66.1 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 112.8 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 187.9 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 286.4 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 319.1 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 279.4 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 176.2 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 154.2 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 110.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 66.1 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 132.2 |
GaN (mp-804) | <1 1 0> | <1 1 -1> | 143.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 176.2 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 154.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 143.4 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 105.8 |
SiO2 (mp-6930) | <0 0 1> | <1 0 -1> | 344.0 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 338.3 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 262.9 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 198.2 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 110.1 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 279.4 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 1> | 319.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 187.9 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 154.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 110.1 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 187.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 263.1 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 319.1 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 286.4 |
ZnSe (mp-1190) | <1 0 0> | <0 1 1> | 319.1 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 279.4 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 176.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 308.4 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 88.1 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 199.5 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 150.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 187.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 211.7 |
CdS (mp-672) | <0 0 1> | <1 0 -1> | 185.2 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 52.9 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 215.1 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 211.7 |
Te2W (mp-22693) | <0 1 0> | <1 0 -1> | 52.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V2CoO6 (mp-557479) | 0.6384 | 0.009 | 3 |
CuMoO4 (mp-619545) | 0.6586 | 0.020 | 3 |
NbSbO4 (mp-3491) | 0.6557 | 0.000 | 3 |
Sb2MoO6 (mp-565786) | 0.6440 | 0.047 | 3 |
V2CoO6 (mp-19311) | 0.6497 | 0.009 | 3 |
Li2VOF4 (mp-764761) | 0.5698 | 0.004 | 4 |
LiNb(OF)2 (mp-769319) | 0.6358 | 0.000 | 4 |
Li2V2O5F2 (mp-765933) | 0.6334 | 0.065 | 4 |
NaV(OF)2 (mp-18953) | 0.5652 | 0.000 | 4 |
V5O12 (mp-777580) | 0.7319 | 0.071 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv O F |
Final Energy/Atom-6.1665 eV |
Corrected Energy-80.1709 eV
-80.1709 eV = -73.9977 eV (uncorrected energy) - 3.3640 eV (MP Advanced Correction) - 2.8092 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)