Final Magnetic Moment27.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.160 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.077 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.07 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi3VO4 + Fe2O3 + VO2 + V3O5 |
Band Gap1.003 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 0> | 196.4 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 285.3 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 253.2 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 285.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 304.7 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 168.8 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 259.0 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 342.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 342.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 243.8 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 285.3 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 171.2 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 285.3 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 121.9 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 121.9 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 60.9 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 171.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 121.9 |
BN (mp-984) | <0 0 1> | <0 0 1> | 304.7 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 182.8 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 1> | 253.2 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 304.7 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 285.3 |
Al (mp-134) | <1 0 0> | <0 0 1> | 243.8 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 304.7 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 228.2 |
SiC (mp-7631) | <1 0 1> | <0 1 1> | 231.2 |
SiC (mp-7631) | <1 0 0> | <1 1 0> | 227.2 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 182.8 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 121.9 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 228.2 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 60.9 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 304.7 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 1> | 253.2 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 182.8 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 304.7 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 304.7 |
C (mp-66) | <1 0 0> | <1 0 1> | 253.2 |
C (mp-66) | <1 1 0> | <0 0 1> | 182.8 |
C (mp-66) | <1 1 1> | <0 0 1> | 182.8 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 228.2 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 57.1 |
Mg (mp-153) | <1 0 1> | <1 0 1> | 168.8 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 342.4 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 243.8 |
Mg (mp-153) | <1 1 0> | <1 1 1> | 259.0 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 182.8 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 0> | 342.4 |
PbS (mp-21276) | <1 1 0> | <1 0 1> | 253.2 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 243.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li(CoO2)2 (mp-771481) | 0.2000 | 0.141 | 3 |
Li(FeO2)2 (mp-771571) | 0.0964 | 0.074 | 3 |
LiCr2O4 (mp-771523) | 0.1544 | 0.038 | 3 |
Co7(SbO6)2 (mp-705595) | 0.2035 | 0.000 | 3 |
LiTi2O4 (mp-776170) | 0.1815 | 0.041 | 3 |
Li4Mn3Cr5O16 (mp-771517) | 0.1070 | 0.039 | 4 |
Li2V3CrO8 (mp-777666) | 0.0956 | 0.027 | 4 |
Li4V5Cr3O16 (mp-777002) | 0.1090 | 0.027 | 4 |
Li4Mn5Fe3O16 (mp-772481) | 0.0842 | 0.054 | 4 |
Li4Cr3Fe5O16 (mp-772464) | 0.1069 | 0.899 | 4 |
Fe3O4 (mp-715491) | 0.3241 | 0.015 | 2 |
Fe3O4 (mp-542433) | 0.3380 | 0.072 | 2 |
Mn3N4 (mp-1080204) | 0.3412 | 0.073 | 2 |
Cr3N4 (mp-1014358) | 0.2753 | 0.227 | 2 |
Fe3O4 (mp-650112) | 0.3095 | 0.057 | 2 |
Li4Mn3Cr3(FeO8)2 (mp-761449) | 0.1066 | 0.570 | 5 |
Li4Ti3Fe3(CuO8)2 (mp-763962) | 0.1089 | 0.084 | 5 |
Li4V3Cr3(FeO8)2 (mp-773698) | 0.0596 | 0.597 | 5 |
Li4Mn3Cr2Co3O16 (mp-769581) | 0.1077 | 0.053 | 5 |
Li4Mn3Cr2Fe3O16 (mp-849471) | 0.0978 | 0.852 | 5 |
Li3MnFeCo(PO4)3 (mp-764931) | 0.6827 | 0.015 | 6 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.6713 | 0.015 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.6766 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.6799 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.6812 | 0.661 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eVFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv V_pv Fe_pv O |
Final Energy/Atom-6.6767 eV |
Corrected Energy-216.8944 eV
-216.8944 eV = -186.9468 eV (uncorrected energy) - 18.7110 eV (MP Advanced Correction) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)