Final Magnetic Moment13.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.141 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.087 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.52 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNi2P2O7 + NbPO5 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [146] |
HallR 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 260.9 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 326.2 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 195.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 195.7 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 65.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 65.2 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 326.2 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 326.2 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 191.3 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 260.9 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 65.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 195.7 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 195.7 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 195.7 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 260.9 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 260.9 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 260.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 260.9 |
BN (mp-984) | <0 0 1> | <0 0 1> | 65.2 |
BN (mp-984) | <1 1 0> | <0 0 1> | 65.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 195.7 |
Al (mp-134) | <1 1 1> | <0 0 1> | 195.7 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 130.5 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 195.7 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 179.8 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 195.7 |
C (mp-66) | <1 1 1> | <0 0 1> | 65.2 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 326.2 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 326.2 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 260.9 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 65.2 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 326.2 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 260.9 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 65.2 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 260.9 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 65.2 |
PbSe (mp-2201) | <1 0 0> | <1 0 1> | 191.3 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 65.2 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 1> | 191.3 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 260.9 |
MoSe2 (mp-1634) | <1 1 0> | <0 0 1> | 260.9 |
Si (mp-149) | <1 1 0> | <0 0 1> | 326.2 |
Si (mp-149) | <1 1 1> | <0 0 1> | 195.7 |
Au (mp-81) | <1 1 1> | <0 0 1> | 260.9 |
CdSe (mp-2691) | <1 0 0> | <1 0 1> | 191.3 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 65.2 |
C (mp-48) | <0 0 1> | <0 0 1> | 195.7 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 260.9 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 260.9 |
WSe2 (mp-1821) | <1 1 1> | <0 0 1> | 260.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnPO4 (mp-773411) | 0.3159 | 0.050 | 3 |
VPO4 (mp-861584) | 0.2060 | 0.076 | 3 |
FePO4 (mp-773675) | 0.3204 | 0.045 | 3 |
TiPO4 (mp-779587) | 0.1812 | 0.077 | 3 |
Fe7(PO5)4 (mp-690584) | 0.3775 | 0.037 | 3 |
NbFe5(PO4)6 (mp-771596) | 0.1083 | 0.017 | 4 |
CrNi5(PO4)6 (mp-772386) | 0.0774 | 0.087 | 4 |
TiFe5(PO4)6 (mp-773598) | 0.1089 | 0.024 | 4 |
TiNi5(PO4)6 (mp-773434) | 0.0998 | 0.084 | 4 |
VFe5(PO4)6 (mp-782634) | 0.1051 | 0.028 | 4 |
VO2 (mp-777469) | 0.7458 | 0.038 | 2 |
VO2 (mvc-6918) | 0.6724 | 0.094 | 2 |
MoO2 (mvc-6944) | 0.6405 | 0.281 | 2 |
MnFe3Co2(PO4)6 (mp-762041) | 0.1046 | 0.036 | 5 |
CrFe3Ni2(PO4)6 (mp-850902) | 0.0973 | 0.030 | 5 |
VFe3Co2(PO4)6 (mp-777311) | 0.1049 | 0.057 | 5 |
NbFe3Ni2(PO4)6 (mp-776895) | 0.0636 | 0.025 | 5 |
Mn3NbNi2(PO4)6 (mp-778276) | 0.0655 | 0.060 | 5 |
Na2Li3Ti3Al(PO4)6 (mp-769078) | 0.5485 | 0.065 | 6 |
NaLi3Ti2Fe2(PO4)6 (mp-850140) | 0.5275 | 0.011 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.5139 | 0.020 | 6 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.3492 | 0.001 | 6 |
Li2Ti2MnCr2(PO4)6 (mp-777244) | 0.4852 | 0.015 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Nb_pv Ni_pv P O |
Final Energy/Atom-6.6562 eV |
Corrected Energy-267.2976 eV
-267.2976 eV = -239.6226 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 10.8200 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)