Final Magnetic Moment0.165 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.975 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.457 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.05 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCoO + Li3NbO4 |
Band Gap1.704 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 1> | 271.7 |
AlN (mp-661) | <1 0 0> | <1 0 -1> | 153.7 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 316.8 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 253.5 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 149.6 |
GaAs (mp-2534) | <1 0 0> | <1 1 -1> | 290.3 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 37.4 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 112.2 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 187.0 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 187.0 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 253.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 316.8 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 149.6 |
SiO2 (mp-6930) | <0 0 1> | <1 1 -1> | 217.7 |
SiO2 (mp-6930) | <1 1 0> | <1 1 -1> | 145.2 |
SiO2 (mp-6930) | <1 1 1> | <1 1 1> | 104.1 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 336.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 -1> | 290.3 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 37.4 |
InAs (mp-20305) | <1 1 0> | <1 1 1> | 104.1 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 336.6 |
ZnSe (mp-1190) | <1 0 0> | <1 1 -1> | 290.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 149.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 205.0 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 187.0 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 307.5 |
CdS (mp-672) | <1 0 1> | <1 0 -1> | 256.2 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 149.6 |
Te2W (mp-22693) | <0 0 1> | <1 1 -1> | 217.7 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 316.8 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 336.6 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 112.2 |
LiF (mp-1138) | <1 1 0> | <1 1 1> | 208.3 |
Te2W (mp-22693) | <0 1 1> | <1 1 -1> | 290.3 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 316.8 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 316.8 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 187.0 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 187.0 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 149.6 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 316.8 |
BN (mp-984) | <0 0 1> | <1 1 -1> | 217.7 |
BN (mp-984) | <1 0 0> | <1 0 0> | 299.2 |
BN (mp-984) | <1 0 1> | <1 0 0> | 224.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 -1> | 290.3 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 190.1 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 316.8 |
Bi2Se3 (mp-541837) | <1 0 0> | <1 0 -1> | 256.2 |
BN (mp-984) | <1 1 0> | <1 0 0> | 261.8 |
Al (mp-134) | <1 0 0> | <1 0 0> | 149.6 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 187.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CuNi9O10 (mp-767305) | 0.1695 | 0.035 | 3 |
InAgSe2 (mp-686712) | 0.1696 | 0.112 | 3 |
LiCr2O3 (mp-770580) | 0.1723 | 0.099 | 3 |
LiFeO2 (mp-771919) | 0.1716 | 0.172 | 3 |
V2NO (mp-690555) | 0.1565 | 0.509 | 3 |
Li3Ti(CoO2)4 (mp-771086) | 0.1082 | 0.070 | 4 |
Li3Ni4SbO8 (mp-774126) | 0.0566 | 0.021 | 4 |
Li3Co4TeO8 (mp-772068) | 0.0983 | 0.112 | 4 |
LiTe3 (mp-27466) | 0.1997 | 0.009 | 2 |
In2Se3 (mp-1068548) | 0.3219 | 0.530 | 2 |
In2Se3 (mp-20830) | 0.3264 | 0.530 | 2 |
SrN (mp-1078609) | 0.3178 | 0.438 | 2 |
Sb2Te3 (mp-1080789) | 0.1899 | 0.129 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.6616 | 0.139 | 5 |
Hg (mp-982872) | 0.3707 | 0.020 | 1 |
Se (mp-7755) | 0.4073 | 0.181 | 1 |
Te (mp-10654) | 0.4046 | 0.047 | 1 |
Te (mp-105) | 0.3032 | 0.047 | 1 |
P (mp-53) | 0.4216 | 0.144 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Nb_pv Co O |
Final Energy/Atom-6.0312 eV |
Corrected Energy-109.6136 eV
-109.6136 eV = -96.4993 eV (uncorrected energy) - 7.4960 eV (MP Advanced Correction) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)