Final Magnetic Moment-0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom-2.824 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.098 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.79 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNb12O29 + TiO2 + LiNbO2 + TiNb3O6 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 150.0 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 75.0 |
InAs (mp-20305) | <1 1 0> | <0 1 1> | 105.7 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 300.0 |
Ni (mp-23) | <1 1 0> | <0 1 1> | 105.7 |
PbSe (mp-2201) | <1 1 0> | <0 1 1> | 105.7 |
BaTiO3 (mp-5986) | <1 0 1> | <0 1 1> | 211.4 |
NdGaO3 (mp-3196) | <1 1 0> | <0 1 0> | 300.0 |
Ga2O3 (mp-886) | <1 1 0> | <0 1 1> | 211.4 |
Au (mp-81) | <1 0 0> | <1 1 1> | 257.9 |
C (mp-48) | <0 0 1> | <0 1 1> | 105.7 |
C (mp-48) | <1 1 0> | <0 1 0> | 300.0 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 300.0 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 225.0 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 105.7 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 300.0 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 150.0 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 211.4 |
Ag (mp-124) | <1 0 0> | <1 1 1> | 257.9 |
Al (mp-134) | <1 1 0> | <0 1 1> | 211.4 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 225.0 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 225.0 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 300.0 |
TeO2 (mp-2125) | <0 1 0> | <0 1 1> | 211.4 |
TeO2 (mp-2125) | <1 0 0> | <0 1 1> | 211.4 |
TeO2 (mp-2125) | <1 1 0> | <0 1 0> | 300.0 |
Fe3O4 (mp-19306) | <1 0 0> | <0 1 0> | 75.0 |
Fe3O4 (mp-19306) | <1 1 0> | <0 1 1> | 105.7 |
Fe3O4 (mp-19306) | <1 1 1> | <1 1 1> | 128.9 |
C (mp-66) | <1 1 1> | <0 1 0> | 225.0 |
LaF3 (mp-905) | <0 0 1> | <0 1 0> | 225.0 |
PbS (mp-21276) | <1 0 0> | <0 1 0> | 75.0 |
PbS (mp-21276) | <1 1 0> | <0 1 1> | 105.7 |
GaP (mp-2490) | <1 0 0> | <0 1 0> | 150.0 |
PbSe (mp-2201) | <1 0 0> | <0 1 0> | 75.0 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 0> | 150.0 |
MoSe2 (mp-1634) | <0 0 1> | <0 1 0> | 300.0 |
Si (mp-149) | <1 0 0> | <0 1 0> | 150.0 |
CdSe (mp-2691) | <1 0 0> | <0 1 0> | 75.0 |
CdSe (mp-2691) | <1 1 0> | <0 1 1> | 105.7 |
WSe2 (mp-1821) | <0 0 1> | <0 1 0> | 300.0 |
NaCl (mp-22862) | <1 0 0> | <0 1 0> | 300.0 |
CaCO3 (mp-3953) | <0 0 1> | <0 1 0> | 225.0 |
CaCO3 (mp-3953) | <1 1 0> | <0 1 0> | 150.0 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <1 0 0> | 150.1 |
SiC (mp-8062) | <1 0 0> | <0 1 0> | 75.0 |
CsI (mp-614603) | <1 0 0> | <0 1 0> | 300.0 |
GaSb (mp-1156) | <1 0 0> | <0 1 0> | 75.0 |
GaSb (mp-1156) | <1 1 0> | <0 1 1> | 105.7 |
SrTiO3 (mp-4651) | <0 0 1> | <0 1 0> | 150.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li11Ti8Fe5O32 (mp-769463) | 0.2726 | 0.035 | 4 |
Li5Ti4Co3O16 (mp-769510) | 0.2812 | 0.096 | 4 |
Li4Nb5V3O16 (mp-770888) | 0.2736 | 0.078 | 4 |
Li11Ti4Fe9O32 (mp-771347) | 0.2651 | 0.057 | 4 |
Li4Ti5Nb3O16 (mp-772157) | 0.2671 | 0.116 | 4 |
Cr3N4 (mp-1014358) | 0.5531 | 0.059 | 2 |
Ge3N4 (mp-641541) | 0.5316 | 0.207 | 2 |
Si3N4 (mp-641539) | 0.5535 | 0.287 | 2 |
Fe3O4 (mp-650112) | 0.4829 | 0.037 | 2 |
Fe3O4 (mp-542433) | 0.5652 | 0.051 | 2 |
MgTi2O4 (mvc-5132) | 0.2937 | 0.059 | 3 |
CaTi2O4 (mvc-5273) | 0.3116 | 0.140 | 3 |
CaTi2O4 (mvc-4945) | 0.3204 | 0.141 | 3 |
Ti2ZnO4 (mvc-5175) | 0.3156 | 0.241 | 3 |
Ca(NiO2)2 (mvc-5741) | 0.3240 | 0.156 | 3 |
Li4V2Cr3Sn3O16 (mp-775525) | 0.2754 | 0.045 | 5 |
Li4Ti2Nb3Cr3O16 (mp-761411) | 0.2691 | 0.096 | 5 |
Li4Nb3Ni3(SbO8)2 (mp-764765) | 0.2544 | 0.135 | 5 |
Li4Fe2Ni3Sn3O16 (mp-775337) | 0.2417 | 0.056 | 5 |
Li4Nb2Co3Sb3O16 (mp-776859) | 0.2544 | 0.100 | 5 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.4069 | 0.030 | 6 |
Li3MnFeCo(PO4)3 (mp-764708) | 0.4195 | 0.012 | 6 |
Li3MnFeCo(PO4)3 (mp-764931) | 0.4314 | 0.015 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.4329 | 0.062 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.4304 | 0.015 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points32 |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Ti_pv Nb_pv O |
Final Energy/Atom-8.2479 eV |
Corrected Energy-484.3533 eV
-484.3533 eV = -461.8801 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)