Final Magnetic Moment0.923 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.930 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.064 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.43 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNa4As2O7 + NaCuO2 + Cu2O3 + Na3B7O12 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 244.4 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 69.8 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 121.2 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 242.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 104.7 |
GaAs (mp-2534) | <1 0 0> | <1 1 1> | 257.0 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 171.3 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 242.3 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 232.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 209.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 211.9 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 1> | 257.0 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 244.4 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 139.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 34.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 314.2 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 174.5 |
ZnSe (mp-1190) | <1 0 0> | <1 1 1> | 257.0 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 339.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 242.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 314.2 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 339.2 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 232.7 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 244.4 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 139.6 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 257.0 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 282.6 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 314.2 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 193.8 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 244.4 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 174.5 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 60.6 |
TePb (mp-19717) | <1 1 1> | <1 0 0> | 302.9 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 302.9 |
Te2Mo (mp-602) | <1 0 1> | <1 1 1> | 171.3 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 349.1 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 314.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 349.1 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 174.5 |
BN (mp-984) | <0 0 1> | <0 0 1> | 244.4 |
BN (mp-984) | <1 0 0> | <0 0 1> | 314.2 |
BN (mp-984) | <1 0 1> | <1 1 1> | 257.0 |
BN (mp-984) | <1 1 0> | <0 1 1> | 298.6 |
SiC (mp-7631) | <1 1 0> | <0 0 1> | 244.4 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 0> | 232.7 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 314.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 244.4 |
Bi2Se3 (mp-541837) | <1 0 1> | <1 1 1> | 257.0 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 279.3 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 139.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na3CrBAsO7 (mp-772378) | 0.3094 | 0.021 | 5 |
Na3FeBAsO7 (mp-771393) | 0.3071 | 0.155 | 5 |
Na3SiBSbO7 (mp-770708) | 0.2703 | 0.080 | 5 |
Na3CuBPO7 (mp-756517) | 0.2041 | 0.067 | 5 |
Na3SiSnBO7 (mp-772986) | 0.2418 | 0.000 | 5 |
Na5LiCo2P2(CO7)2 (mp-761297) | 0.4833 | 0.013 | 6 |
Na5LiNi2P2(CO7)2 (mp-770324) | 0.4243 | 0.009 | 6 |
Na5LiFe2P2(CO7)2 (mp-769718) | 0.5065 | 0.000 | 6 |
Na2LiFePCO7 (mp-773705) | 0.4454 | 0.138 | 6 |
Na5LiNi2P2(CO7)2 (mp-771060) | 0.4753 | 0.011 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Cu_pv B As O |
Final Energy/Atom-5.7064 eV |
Corrected Energy-157.9855 eV
Uncorrected energy = -148.3675 eV
Composition-based energy adjustment (-0.687 eV/atom x 14.0 atoms) = -9.6180 eV
Corrected energy = -157.9855 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)